Abstract: The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpendicular direction). The optimal extruding technological parameter has been given in different extruding technology by the physical simulation (H: 300℃, 550kN, 0.16mm. P: 300℃, 215kN, 0.16mm). The effect on the coating speed by other extruding technological parameters in the different extruding technology has been discussed. The extruding temperature and extruding force is higher, the coating speed is faster. It has been pointed, that the affection on the extruding technology by the extruding temperature has also behaved as the extruding temperature rising up spontaneously. The reason for exiting the minimum extruding force and maximum extruding force also has been discussion in this paper. It is also important to the extruding process and coating speed that is the coating clearance.

详情信息展示

THE PHYSICAL SIMULATION ON EXTRUSION PROCESS OF GLASS FIBER COMPOSITE WIRE COATED BY LEAD

F.Han1,H.F.Sun1,W.B.Fang1,W.X.He1,E.D.Wang1

(1.School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China)

Abstract:The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpendicular direction). The optimal extruding technological parameter has been given in different extruding technology by the physical simulation (H: 300℃, 550kN, 0.16mm. P: 300℃, 215kN, 0.16mm). The effect on the coating speed by other extruding technological parameters in the different extruding technology has been discussed. The extruding temperature and extruding force is higher, the coating speed is faster. It has been pointed, that the affection on the extruding technology by the extruding temperature has also behaved as the extruding temperature rising up spontaneously. The reason for exiting the minimum extruding force and maximum extruding force also has been discussion in this paper. It is also important to the extruding process and coating speed that is the coating clearance.

Key words:composite; lead; glass fiber; coating; physical simulation;

【全文内容正在添加中】

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号