Effect of minor boron addition on mechanical properties of wrought TiAl alloy

来源期刊:中国有色金属学报(英文版)2000年第2期

论文作者:王瑜 林栋梁 Chi C.LA W

文章页码:162 - 166

Key words:titanium aluminide; intermetallics; boron

Abstract: The effect of minor boron(1.0%, mole fraction) addition on tensile properties of wrought Ti-47-2Mn-2Nb alloy was investigated within the temperature range from 77K to 1373K and the strain rate range from 10-5 s-1 to 10-1 s-1 . It was found that the minor addition of boron effectively refines the nearly lamellar microstructure of the alloy, significantly improves its strength, as well as its ductility. Although to a less degree, below its brittle-to-ductile transition temperature (TBD), it does not harm its strength above its TBD, and is therefore proved to be an potentially effective way to improve comprehensive properties of wrought TiAl alloy. The B addition was also found to produce no obvious change in the fracture mode except for the cases around TBD.

详情信息展示

 

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号