Volcanic Activity and Thermal Excitation of Rich-silicon Iron Ore Tailing in Concrete

来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2017年第2期

论文作者:周明凯 ZHU Zhigang 李北星 LIU Jincheng

文章页码:365 - 372

摘    要:In order to distinguish the filling effect and volcanic activity and explore the ways motivating the activity of rich-silicon iron ore tailing(IOT), inert quartz was brought in as the correction standard, the influences of fineness, calcination, thermal curing system and some other factors were investigated by IR, XRD, MIP, and so on microscopic methods. The experimental results show grinding and calcination can only change the amorphous state of SiO2, and IOT do not have volcanic activity in concrete cured under room temperature condition. Thermal curing systems can stimulate the activity of IOT, especially mortar cured by autoclave curing system can consume a large amount of Ca(OH)2 and hard calcium silicate and has a closer structure. When the specific surface area of IOT powder is 800 m2/kg, and 30% cement is replaced by IOT powder, the mortar strength with IOT powder is even higher than that with cementonly.

详情信息展示

Volcanic Activity and Thermal Excitation of Rich-silicon Iron Ore Tailing in Concrete

周明凯,ZHU Zhigang,李北星,LIU Jincheng

State Key Laboratory of Silicate Materials for Architecture,Wuhan University of Technology

摘 要:In order to distinguish the filling effect and volcanic activity and explore the ways motivating the activity of rich-silicon iron ore tailing(IOT), inert quartz was brought in as the correction standard, the influences of fineness, calcination, thermal curing system and some other factors were investigated by IR, XRD, MIP, and so on microscopic methods. The experimental results show grinding and calcination can only change the amorphous state of SiO2, and IOT do not have volcanic activity in concrete cured under room temperature condition. Thermal curing systems can stimulate the activity of IOT, especially mortar cured by autoclave curing system can consume a large amount of Ca(OH)2 and hard calcium silicate and has a closer structure. When the specific surface area of IOT powder is 800 m2/kg, and 30% cement is replaced by IOT powder, the mortar strength with IOT powder is even higher than that with cementonly.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号