The Stability of Rare Earth-Iron-Nitrides Sm2(Fe,M)17Ny,Permanent Magnets
来源期刊:Journal of Rare Earths1993年第1期
论文作者:杨俊 周寿增 张茂才 马德青 李佛标 王润
文章页码:69 - 71
摘 要:<正> The effects of the partial substitution of element M(M=Cr,V,Mn,x=0.05;Zr,Ga,x=0.017;Si,x=0.15;Co,x=0.10)for Fe in samarium-iron-nitride Sm2(Fe1-xMx)17Ny compounds on their stabilitiesand Curie temperatures have been studied.It is found that Co,Ga can raise the Curie temperature of thecompounds.The initial decomposition temperatures cannot be raised significantly by all the studied elementsexcept Co.The result contradicts the formation enthalpy consideration.The final decomposition tempera-tures can be raised by all of the substitution elements.The effects of atmospheres on their decomposition be-havior were also studied.The results show that oxidation is the major reason for magnetic deterioration ofthe powder heated in air.Compared with nitrogen atmosphere,argon or vacuum helps to delay the decompo-sition of the compounds.
杨俊,周寿增,张茂才,马德青,李佛标,王润
摘 要:<正> The effects of the partial substitution of element M(M=Cr,V,Mn,x=0.05;Zr,Ga,x=0.017;Si,x=0.15;Co,x=0.10)for Fe in samarium-iron-nitride Sm2(Fe1-xMx)17Ny compounds on their stabilitiesand Curie temperatures have been studied.It is found that Co,Ga can raise the Curie temperature of thecompounds.The initial decomposition temperatures cannot be raised significantly by all the studied elementsexcept Co.The result contradicts the formation enthalpy consideration.The final decomposition tempera-tures can be raised by all of the substitution elements.The effects of atmospheres on their decomposition be-havior were also studied.The results show that oxidation is the major reason for magnetic deterioration ofthe powder heated in air.Compared with nitrogen atmosphere,argon or vacuum helps to delay the decompo-sition of the compounds.
关键词: