Preparation of fibrous nickel oxide particles

来源期刊:中国有色金属学报(英文版)2003年第6期

论文作者:张传福 湛菁 邬建辉 郭学益 M. Okido

文章页码:1440 - 1445

Key words:chemical precipitation and pyrolysis; precursor; fibrous NiO particles; preparation

Abstract: The fibrous nickel oxide particles were prepared by chemical precipitation and pyrolysis method. The NiO precursors were firstly precipitated from nickel ions solution with addition of oxalate salt, and then the final NiO particles were obtained by pyrolysis of the precursor. The effects of the pH value, precipitation temperature, reactant concentration, addition of surfactant on the morphology of the precursor particles were investigated. The crystallinity, purity, morphology of the fibrous NiO were analyzed by XRD and SEM. The fibrous NiO particles with 100-120 in axis/diameter ratio may be produced under the optimal process conditions that are proposed: the Ni2+ concentration is 0.5-0.8mol/L, pH value is 8.3-8.9, precipitation temperature is 60-75℃, pyrolysis temperature is 500-600℃.

详情信息展示

 

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号