Tribological Behavior of Al CoCrFeNi(Ti0.5) High Entropy Alloys under Oil and MACs Lubrication

来源期刊:JOURNAL OF MATERIALS SCIENCE TECHNOLOG2016年第5期

论文作者:Yuan Yu Jun Wang Jinshan Li Jun Yang Hongchao Kou Weimin Liu

文章页码:470 - 476

摘    要:The tribological properties of AlCoCrFeNi and AlCoCrFeNiTi0.5 high entropy alloys under gear oil and multiply alkylated cyclopentanes(MACs)lubrication condition have been studied.The equiaxed crystal structure of AlCoCrFeNi alloy is obtained after heat-treatment.The AlCoCrFeNiTi0.5 alloy keeps dendrite structure.Under the gear oil with good lubrication action,AlCoCrFeNiTi0.5 alloy preserves better tribological properties than AlCoCrFeNi alloy.The delamination and crack behaviors tend to occur in the grain boundary of AlCoCrFeNi alloy and along the interdendrite region of AlCoCrFeNiTi0.5 alloy.Under the MACs with relatively poor lubrication action,the applied load slightly influences the wear behavior of AlCoCrFeNi alloy,but seriously impacts the wear mechanism of AlCoCrFeNiTi0.5 alloy.Compared with AlCoCrFeNi alloy,AlCoCrFeNiTi0.5 alloy keeps better wear-resistance at low applied load of 100 N,but preserves less wearresistance at high applied load of 200 N.

详情信息展示

Tribological Behavior of Al CoCrFeNi(Ti0.5) High Entropy Alloys under Oil and MACs Lubrication

Yuan Yu1,Jun Wang1,Jinshan Li1,Jun Yang2,Hongchao Kou1,Weimin Liu2

1. State Key Laboratory of Solidification Processing, Northwestern Polytechnical University2. State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences

摘 要:The tribological properties of AlCoCrFeNi and AlCoCrFeNiTi0.5 high entropy alloys under gear oil and multiply alkylated cyclopentanes(MACs)lubrication condition have been studied.The equiaxed crystal structure of AlCoCrFeNi alloy is obtained after heat-treatment.The AlCoCrFeNiTi0.5 alloy keeps dendrite structure.Under the gear oil with good lubrication action,AlCoCrFeNiTi0.5 alloy preserves better tribological properties than AlCoCrFeNi alloy.The delamination and crack behaviors tend to occur in the grain boundary of AlCoCrFeNi alloy and along the interdendrite region of AlCoCrFeNiTi0.5 alloy.Under the MACs with relatively poor lubrication action,the applied load slightly influences the wear behavior of AlCoCrFeNi alloy,but seriously impacts the wear mechanism of AlCoCrFeNiTi0.5 alloy.Compared with AlCoCrFeNi alloy,AlCoCrFeNiTi0.5 alloy keeps better wear-resistance at low applied load of 100 N,but preserves less wearresistance at high applied load of 200 N.

关键词:

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号