Liquid-liquid extraction and separation of total rare earth(RE) metals from polymetallic manganese nodule leaching solution

来源期刊:JOURNAL OF RARE EARTHS2015年第2期

论文作者:P.K.Parhi K.H.Park C.W.Nam J.T.Park

文章页码:207 - 213

摘    要:The study on the solvent extraction for quantitative and selective separation of total rare earth metals from the polymetallic nodule leach liquor was investigated. The typical leach liquor bearing 0. 094 g/L total rare earth, 0. 23 g/L Mn, 0.697 g/L Cu, 0.2 g/L Fe, 0.01 g/L Co and 0.735 g/L Ni was subjected to the removal iron content by precipitation method using Ca(OH)2 at pH 3.95, prior to solvent extraction of rare earth metals. Three different organo-phosphoric acid reagents(D2EHPA, PC88 A, Cyanex 272) were used to ascertain their performances and selectivity towards the loading of rare earth metals in presence of other base metals. Based on the results of eq. pH effect, the performances of above three extractants followed the order as: D2EHPA>PC88A>Cyanex 272. To ensure the absence of extraction of base metals(Cu, Co, Ni), the eq. pH of the solution was optimized at the level of 2.21, though higher rare earth metal extraction efficiency was observed at higher eq. pH with either of the extractants. The complete process flow diagram for substantial recovery of total rare earth was developed using D2 EHPA. Extraction isotherm plot was constructed at A:O=12:1, 3-stages and pHe=2.21, using 0.8 mol/L D2 EHPA and the predicted condition of this study was further confirmed by 6-Cycles Counter Current Simulation(CCS) study. The stripping of total rare earth from loaded organic phase(LO) was conducted using HCl solution. Mc-Cabe Thiele diagram study carried out at A:O=1:5 using 4 mol/L HCl showed that three theoretical stages were needed for quantitative stripping of total rare earth. The subsequent stripped solution resulted thus led to contain total rare earth of 5.6 g/L indicating a very high enrichment of total metals by solvent extraction(SX) process.

详情信息展示

Liquid-liquid extraction and separation of total rare earth(RE) metals from polymetallic manganese nodule leaching solution

P.K.Parhi1,2,K.H.Park1,C.W.Nam1,J.T.Park1

1. Mineral Resources Research Division, Korea Institute of Geoscience & Mineral Resources (KIGAM),Daejeon 305-350, Republic of Korea2. School of Applied Science and Center of Industrial Technology, KIIT University,Bhubaneswar 751024, Odisha, India

摘 要:The study on the solvent extraction for quantitative and selective separation of total rare earth metals from the polymetallic nodule leach liquor was investigated. The typical leach liquor bearing 0. 094 g/L total rare earth, 0. 23 g/L Mn, 0.697 g/L Cu, 0.2 g/L Fe, 0.01 g/L Co and 0.735 g/L Ni was subjected to the removal iron content by precipitation method using Ca(OH)2 at pH 3.95, prior to solvent extraction of rare earth metals. Three different organo-phosphoric acid reagents(D2EHPA, PC88 A, Cyanex 272) were used to ascertain their performances and selectivity towards the loading of rare earth metals in presence of other base metals. Based on the results of eq. pH effect, the performances of above three extractants followed the order as: D2EHPA>PC88A>Cyanex 272. To ensure the absence of extraction of base metals(Cu, Co, Ni), the eq. pH of the solution was optimized at the level of 2.21, though higher rare earth metal extraction efficiency was observed at higher eq. pH with either of the extractants. The complete process flow diagram for substantial recovery of total rare earth was developed using D2 EHPA. Extraction isotherm plot was constructed at A:O=12:1, 3-stages and pHe=2.21, using 0.8 mol/L D2 EHPA and the predicted condition of this study was further confirmed by 6-Cycles Counter Current Simulation(CCS) study. The stripping of total rare earth from loaded organic phase(LO) was conducted using HCl solution. Mc-Cabe Thiele diagram study carried out at A:O=1:5 using 4 mol/L HCl showed that three theoretical stages were needed for quantitative stripping of total rare earth. The subsequent stripped solution resulted thus led to contain total rare earth of 5.6 g/L indicating a very high enrichment of total metals by solvent extraction(SX) process.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号