简介概要

Heat Treatment Properties of 42CrMo Steel for Bearing Ring of Varisized Shield Tunneling Machine

来源期刊:Acta Metallurgica Sinica2014年第3期

论文作者:Bo Jiang Leyu Zhou Xinli Wen Chaolei Zhang Yazheng Liu

文章页码:383 - 388

摘    要:The heat treatment properties of 42 CrMo steel for bearing ring of varisized shield tunneling machine were investigated by optical microscope(OM), scanning electron microscope(SEM), transmission electron microscope(TEM),and impact tests. The addition of 0.03 wt% C into 42 CrMo steel can increase the hardness. But it reduces the impact energy by 46 J because of the appearance of coarser carbides in the matrix and the carbides along the austenite grain boundary.The addition of 0.40 wt% Mn into 42 CrMo steel can improve hardenability. However, the toughness of steel is also reduced by 26 J mainly because of the coarsening of carbides and the strengthening of matrix. Both hardenability and toughness of 42 CrMo steel can be improved by adding 1.49 wt% Ni and reducing 0.32 wt% Cr. The depth of hardening layer can be raised to 45 mm, and the impact energy at-20 °C is 120 J. Thus, it is concluded that a good combination of hardness, hardenability, and toughness of 42 CrMo steel can be achieved by alloying with adding some content of C and Ni.Detailed content of C and Ni should be on the requirements of heat treatment properties of steel for bearing ring of varisized shield tunneling machine.

详情信息展示

Heat Treatment Properties of 42CrMo Steel for Bearing Ring of Varisized Shield Tunneling Machine

Bo Jiang,Leyu Zhou,Xinli Wen,Chaolei Zhang,Yazheng Liu

School of Materials Science and Engineering, University of Science and Technology Beijing

摘 要:The heat treatment properties of 42 CrMo steel for bearing ring of varisized shield tunneling machine were investigated by optical microscope(OM), scanning electron microscope(SEM), transmission electron microscope(TEM),and impact tests. The addition of 0.03 wt% C into 42 CrMo steel can increase the hardness. But it reduces the impact energy by 46 J because of the appearance of coarser carbides in the matrix and the carbides along the austenite grain boundary.The addition of 0.40 wt% Mn into 42 CrMo steel can improve hardenability. However, the toughness of steel is also reduced by 26 J mainly because of the coarsening of carbides and the strengthening of matrix. Both hardenability and toughness of 42 CrMo steel can be improved by adding 1.49 wt% Ni and reducing 0.32 wt% Cr. The depth of hardening layer can be raised to 45 mm, and the impact energy at-20 °C is 120 J. Thus, it is concluded that a good combination of hardness, hardenability, and toughness of 42 CrMo steel can be achieved by alloying with adding some content of C and Ni.Detailed content of C and Ni should be on the requirements of heat treatment properties of steel for bearing ring of varisized shield tunneling machine.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号