Synthesis of CaWO4:Eu3+ phosphor powders via ethylene glycol route and its optical properties

来源期刊:JOURNAL OF RARE EARTHS2012年第4期

论文作者:K.Gayatri Sharma N.Rajmuhon Singh

文章页码:310 - 314

摘    要:Eu3+ doped CaWO4 with tetragonal system were prepared at comparatively low temperature (125 ?C) in ethylene glycol medium. The phosphor was further investigated by X-ray diffractometer (XRD), photoluminescence spectrophotometer (PL), Fourier transform infra red (FT-IR) spectroscopy and transmission electron microscopy (TEM). XRD analysis indicated a decrease in the unit cell volume of CaWO4 with increasing Eu3+ ion concentration. It indicated the homogeneous substitution of Ca2+ ions in CaWO4 by the Eu3+ ions. TEM images showed that the particle size ranged from 20 to 200 nm and it could extend the application of the nanoparticles. The photoluminescence study showed that the intensity of electric dipole transition (5D0→7F2) at 614 nm dominated over the magnetic dipole transition (5D0→7F1) at 592 nm. The optimum concentration of Eu3+ for the highest luminescence was found to be 20 at.%. The as prepared samples were found to be dis-persible in water and methanol.

详情信息展示

Synthesis of CaWO4:Eu3+ phosphor powders via ethylene glycol route and its optical properties

K.Gayatri Sharma,N.Rajmuhon Singh

Department of Chemistry, Manipur University, Canchipur-795003, Imphal, Manipur, India

摘 要:Eu3+ doped CaWO4 with tetragonal system were prepared at comparatively low temperature (125 ?C) in ethylene glycol medium. The phosphor was further investigated by X-ray diffractometer (XRD), photoluminescence spectrophotometer (PL), Fourier transform infra red (FT-IR) spectroscopy and transmission electron microscopy (TEM). XRD analysis indicated a decrease in the unit cell volume of CaWO4 with increasing Eu3+ ion concentration. It indicated the homogeneous substitution of Ca2+ ions in CaWO4 by the Eu3+ ions. TEM images showed that the particle size ranged from 20 to 200 nm and it could extend the application of the nanoparticles. The photoluminescence study showed that the intensity of electric dipole transition (5D0→7F2) at 614 nm dominated over the magnetic dipole transition (5D0→7F1) at 592 nm. The optimum concentration of Eu3+ for the highest luminescence was found to be 20 at.%. The as prepared samples were found to be dis-persible in water and methanol.

关键词:

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号