Preparation and Characteristics of Hydroxyapatite Whiskers by Homogeneous Precipitation Method
来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2001年第3期
论文作者:王友法
文章页码:19 - 22
摘 要:Hydroxyapatite whiskers were prepared by the homogeneous precipitation method. Soluble calcium ion and phosphate ion were used as initial materials, they were refluxed respectively at 85℃ , 90℃ and 95℃ for various lengths of time. A proper precipitation agent was selected to control the releasing speed of ions in the system; it induced the hydraxyapatite crystal to grow in a desired way. The pH values of each solutions were measured continuously during the reaction. After the reaction, the products were characterized by X- ray powder dif-fractometry (XRD), scanning electron microscopy ( SEM) and infrared spectroscopy (IR). It is shown that long hydroxyapatite whiskers were obtained under the conditions of 95℃ - 48h and 90℃ - 12h, 85℃ - 120h.
王友法
摘 要:Hydroxyapatite whiskers were prepared by the homogeneous precipitation method. Soluble calcium ion and phosphate ion were used as initial materials, they were refluxed respectively at 85℃ , 90℃ and 95℃ for various lengths of time. A proper precipitation agent was selected to control the releasing speed of ions in the system; it induced the hydraxyapatite crystal to grow in a desired way. The pH values of each solutions were measured continuously during the reaction. After the reaction, the products were characterized by X- ray powder dif-fractometry (XRD), scanning electron microscopy ( SEM) and infrared spectroscopy (IR). It is shown that long hydroxyapatite whiskers were obtained under the conditions of 95℃ - 48h and 90℃ - 12h, 85℃ - 120h.
关键词: