Abstract: Al-10Pb (in mass fraction) and Al-20Pb mixed powders were mechanically milled. The morphology and the microstructures of the milled powders were observed by scanning electron microscopy and electron probe microscopy, and the microhardness and density of the milled powder were tested. The results show that at beginning of milling, the particle size of Al-Pb mixed powder increases, then it decreases to a stable value. Mechanical milling leads to the formation of laminar structure. With prolonging milling time, the laminar structure is refined, finally fractures to small particles; the hardness of Al-Pb powder is increased and the compact density is decreased. Compared with Al-10Pb powder, Al-20Pb powder has obvious laminar structure, low hardness, and high density.

详情信息展示

Variation of mechanical properties and microstructures of Al-Pb mixed powder during mechanical milling

HE Wen-xiong(贺文雄)1, FANG Wen-bin(房文斌)1, WANG Er-de(王尔德)1,2, HAN Fei(韩 飞)1

(1. Research Institute for Materials,
Harbin Institute of Technology, Harbin 150001, China;
2. School of Materials Science and Engineering,
Harbin Institute of Technology, Harbin 150001, China)

Abstract:Al-10Pb (in mass fraction) and Al-20Pb mixed powders were mechanically milled. The morphology and the microstructures of the milled powders were observed by scanning electron microscopy and electron probe microscopy, and the microhardness and density of the milled powder were tested. The results show that at beginning of milling, the particle size of Al-Pb mixed powder increases, then it decreases to a stable value. Mechanical milling leads to the formation of laminar structure. With prolonging milling time, the laminar structure is refined, finally fractures to small particles; the hardness of Al-Pb powder is increased and the compact density is decreased. Compared with Al-10Pb powder, Al-20Pb powder has obvious laminar structure, low hardness, and high density.

Key words:mechanical milling; Al-Pb alloy; laminar structure

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号