Dendritic and spherical crystal reinforced metallic glass matrix composites

来源期刊:International Journal of Minerals Metallurgy and Materials2013年第4期

论文作者:Jun-wei Qiao Yong Zhang Hui-jun Yang Sheng-bo Sang

文章页码:386 - 392

摘    要:Zr-based bulk metallic glass matrix composites (BMGMCs) with a composition of Zr60.0Ti14.7Nb5.3Cu5.6Ni4.4Be 10.0 (at%) were fabricated by an innovative process, i.e., semisolid processing plus Bridgman solidification. Different morphologies, distributions, and volume fractions of the crystalline phases can be achieved by tailoring the withdrawal velocity. The largest fracture strain of Zr60.0Ti14.7Nb5.3Cu5.6Ni4.4Be10.0(at%) composites with the withdrawal velocity of 1.0 mm/s was found to be 16.7%. The mechanism of plasticity improvement is mainly attributed to the interpenetrated structure of the crystalline phase, which greatly confines the rapid propagation of shear bands.

详情信息展示

Dendritic and spherical crystal reinforced metallic glass matrix composites

Jun-wei Qiao1,2,Yong Zhang3,Hui-jun Yang1,2,Sheng-bo Sang4

1. Laboratory of Applied Physics and Mechanics of Advanced Materials, College of Materials Science and Engineering, Taiyuan University of Technology2. Key Laboratory of Interface Science and Engineering in Advanced Materials (Ministry of Education), Taiyuan University of Technology3. State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing4. MicroNano System Research Center, Taiyuan University of Technology

摘 要:Zr-based bulk metallic glass matrix composites (BMGMCs) with a composition of Zr60.0Ti14.7Nb5.3Cu5.6Ni4.4Be 10.0 (at%) were fabricated by an innovative process, i.e., semisolid processing plus Bridgman solidification. Different morphologies, distributions, and volume fractions of the crystalline phases can be achieved by tailoring the withdrawal velocity. The largest fracture strain of Zr60.0Ti14.7Nb5.3Cu5.6Ni4.4Be10.0(at%) composites with the withdrawal velocity of 1.0 mm/s was found to be 16.7%. The mechanism of plasticity improvement is mainly attributed to the interpenetrated structure of the crystalline phase, which greatly confines the rapid propagation of shear bands.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号