Cerium-Based Sealing Treatment of Mg–Al Hydrotalcite Film on AZ91D Magnesium Alloy

来源期刊:Acta Metallurgica Sinica2016年第11期

论文作者:Qiang-Sheng Dong Zhi-Xin Ba Zhang-Zhong Wang Juan Kuang Zheng-Yang Cai Chen Yuan

文章页码:993 - 1000

摘    要:An environment-friendly cerium-based sealing treatment was developed to improve the surface integrity and corrosion resistance of Mg–Al hydrotalcite film on AZ91D magnesium alloy. The cerium dioxide was generated through three stages namely nucleation, growth and dissolution, modifying the surface of AZ91D Mg alloy, and the hydrotalcite film became integral after being treated for 30 min. The results of polarization curves showed that the anti-corrosive performance of the hydrotalcite film was enhanced by the sealing treatment. Moreover, the immersion tests and electrochemical impedance spectrum measurements also demonstrated that the sealed hydrotalcite film provided a longer-term protection of magnesium alloy from corrosion as compared to the unsealed one.

详情信息展示

Cerium-Based Sealing Treatment of Mg–Al Hydrotalcite Film on AZ91D Magnesium Alloy

Qiang-Sheng Dong1,2,Zhi-Xin Ba1,2,Zhang-Zhong Wang1,2,Juan Kuang1,Zheng-Yang Cai1,Chen Yuan1

1. School of Materials Science and Engineering, Nanjing Institute of Technology2. Jiangsu Key Laboratory of Advanced Structural Materials and Application Technology

摘 要:An environment-friendly cerium-based sealing treatment was developed to improve the surface integrity and corrosion resistance of Mg–Al hydrotalcite film on AZ91D magnesium alloy. The cerium dioxide was generated through three stages namely nucleation, growth and dissolution, modifying the surface of AZ91D Mg alloy, and the hydrotalcite film became integral after being treated for 30 min. The results of polarization curves showed that the anti-corrosive performance of the hydrotalcite film was enhanced by the sealing treatment. Moreover, the immersion tests and electrochemical impedance spectrum measurements also demonstrated that the sealed hydrotalcite film provided a longer-term protection of magnesium alloy from corrosion as compared to the unsealed one.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号