连续冷却过程中铜含量对析出的影响

来源期刊:钢铁2011年第8期

论文作者:李闯 王学敏 尚成嘉 贺信莱

文章页码:73 - 77

关键词:铜含量; 连续冷却; 中间淬火

Key words:Cu content; continuous cooling; intermediate quenching

摘    要:研究了一系列含铜钢在连续冷却过程中的析出行为。采用1℃/s的冷却速度以及中间淬火取样方法获得铁素体组织。利用金相显微镜和透射电镜研究不同铜含量对析出的影响。结果表明:当铜的质量分数高于1.5%时,随着铁素体的产生,在铁素体内产生第二相析出颗粒。当铜的质量分数低于1%时,并未观察到第二相析出。第二相析出物为富铜颗粒,以相间沉淀方式析出。

Abstract: The precipitation behavior of Cu-bearing steels during continuous cooling was investigated.Microstructure of ferrite was obtained by using 1℃/s cooling rates and interrupted cooling.The optical microscope and TEM were used to study the effect of different Cu content on the precipitation process.The results show that when the steels was cooled at 1℃/s,the second-phase precipitates occurs in the steels which Cu content is higher than 1.5%.However there are no obvious precipitates in the steels which Cu content is lower than 1%.The second-phase precipitates are copper-rich particles in the way of phase precipitation.

详情信息展示

连续冷却过程中铜含量对析出的影响

李闯1,王学敏1,尚成嘉1,贺信莱1

(1.北京市北京科技大学材料科学与工程学院)

摘 要:研究了一系列含铜钢在连续冷却过程中的析出行为。采用1℃/s的冷却速度以及中间淬火取样方法获得铁素体组织。利用金相显微镜和透射电镜研究不同铜含量对析出的影响。结果表明:当铜的质量分数高于1.5%时,随着铁素体的产生,在铁素体内产生第二相析出颗粒。当铜的质量分数低于1%时,并未观察到第二相析出。第二相析出物为富铜颗粒,以相间沉淀方式析出。

关键词:铜含量; 连续冷却; 中间淬火

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号