简介概要

Upgradation of bauxite by molecular hydrogen and hydrogen plasma

来源期刊:International Journal of Minerals Metallurgy and Materials2016年第10期

论文作者:B.R.Parhi S.K.Sahoo S.C.Mishra

文章页码:1141 - 1149

摘    要:An approach was developed to upgrade the bauxite ore by molecular hydrogen and hydrogen plasma. A gibbsite-type bauxite sample was obtained from National Aluminium Company(NALCO), Odisha, India. The obtained sample was crushed and sieved(to 100 μm) prior to the chemical analysis and grain-size distribution study. The bauxite sample was calcined in the temperature range from 500 to 700°C for different time intervals to optimize the conditions for maximum moisture removal. This process was followed by the reduction of the calcined ore by molecular hydrogen and hydrogen plasma. Extraction of alumina from the reduced ore was carried out via acid leaching in chloride media for 2 h at 60°C. X-ray diffraction, scanning electron microscopy, thermogravimetry in conjunction with differential scanning calorimetry, and Fourier transform infrared spectroscopy were used to determine the physicochemical characteristics of the material before and after extraction. Alumina extracted from the reduced ore at the optimum calcination temperature of 700°C and the optimum calcination time of 4 h is found to be 90% pure.

详情信息展示

Upgradation of bauxite by molecular hydrogen and hydrogen plasma

B.R.Parhi1,S.K.Sahoo1,S.C.Mishra1

1. Department of Metallurgical and Materials Engineering, National Institute of Technology

摘 要:An approach was developed to upgrade the bauxite ore by molecular hydrogen and hydrogen plasma. A gibbsite-type bauxite sample was obtained from National Aluminium Company(NALCO), Odisha, India. The obtained sample was crushed and sieved(to 100 μm) prior to the chemical analysis and grain-size distribution study. The bauxite sample was calcined in the temperature range from 500 to 700°C for different time intervals to optimize the conditions for maximum moisture removal. This process was followed by the reduction of the calcined ore by molecular hydrogen and hydrogen plasma. Extraction of alumina from the reduced ore was carried out via acid leaching in chloride media for 2 h at 60°C. X-ray diffraction, scanning electron microscopy, thermogravimetry in conjunction with differential scanning calorimetry, and Fourier transform infrared spectroscopy were used to determine the physicochemical characteristics of the material before and after extraction. Alumina extracted from the reduced ore at the optimum calcination temperature of 700°C and the optimum calcination time of 4 h is found to be 90% pure.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号