摘    要:Influences of Sn and Y on the microstructure, mechanical properties, and corrosion behavior of as-cast Mg-5 Li-3 Al-2 Zn(LAZ532) alloy were investigated. The addition of Sn and Y refines grains and results in the formation of Mg2 Sn and Al2 Y phases, thus improving the mechanical properties of alloy by second phase strengthening and grain refinement strengthening. As-cast LAZ532 alloy shows typical filiform corrosion morphology, and the addition of Sn and Y does not change the corrosion mode of alloy. Ascast LAZ532-0.8 Sn-1.2 Y alloy shows excellent mechanical properties with yield strength of 166.2 MPa,ultimate tensile strength of 228.6 MPa and elongation of 14.8 %, and exhibits the best corrosion resistance with the smallest corrosion current density and the lowest anodic dissolution rate.

详情信息展示

Microstructural evolution, mechanical properties and corrosion behavior of as-cast Mg-5Li-3Al-2Zn alloy with different Sn and Y addition

Xiang Peng,Shihao Xu,Dehua Ding,Guanglan Liao,Guohua Wu,Wencai Liu,Wenjiang Ding

National Engineering Research Center of Light Alloy Net Forming and State Key Laboratory of Metal Matrix Composite, School of Materials Science and Engineering, Shanghai Jiao Tong University

摘 要:Influences of Sn and Y on the microstructure, mechanical properties, and corrosion behavior of as-cast Mg-5 Li-3 Al-2 Zn(LAZ532) alloy were investigated. The addition of Sn and Y refines grains and results in the formation of Mg2 Sn and Al2 Y phases, thus improving the mechanical properties of alloy by second phase strengthening and grain refinement strengthening. As-cast LAZ532 alloy shows typical filiform corrosion morphology, and the addition of Sn and Y does not change the corrosion mode of alloy. Ascast LAZ532-0.8 Sn-1.2 Y alloy shows excellent mechanical properties with yield strength of 166.2 MPa,ultimate tensile strength of 228.6 MPa and elongation of 14.8 %, and exhibits the best corrosion resistance with the smallest corrosion current density and the lowest anodic dissolution rate.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号