简介概要

耐候钢异型坯连铸结晶器保护渣性能优化研究

来源期刊:钢铁2009年第9期

论文作者:孙维 汪开忠 文光华 唐萍 刘慧

文章页码:28 - 32

关键词:连铸; 异型坯; 结晶器保护渣; 耐候钢

Key words:continuous casting; beam blank; mould powder; weathering steel

摘    要:由于异型坯形状复杂,在浇注耐候钢的过程中,铸坯表面质量较差,并经常发生粘结漏钢事故。通过实验室研究和工业性试验相结合的方法,根据异型坯连铸耐候钢的特点,分析了耐候钢异型坯表面质量差和浇注过程中发生粘结性漏钢的原因,提出了异型坯连铸耐候钢保护渣优化设计思路,重点研究了协调保护渣润滑和传热性能的影响因素。根据研究结果配制的异型坯连铸耐候钢专用保护渣,大生产应用结果表明,连浇炉数达到10炉以上,未发生粘结漏钢事故,耐候钢异型坯表面质量也有了明显提高。

Abstract: Because the shape of beam blank is complex,the surface quality of beam blank is bad,and the breakout is often occurred.The method combined research in lab with study on industrial scene is adopted,and the character of weathering steel beam blank continuous casting is researched.The surface quality of beam blank and the reasons of sticking breakout of beam blank continuous casting are analyzed.On the basis of these results,the designing plan of weathering steel mould powder is came up with,and the relationship between lubrication and heat transfer is researched.This kind of mould powder is applied in beam blank continuous casting machine,and the continuous casting heats are over 10,there is no breakout,and the surface quality of beam blank is also improved.

详情信息展示

耐候钢异型坯连铸结晶器保护渣性能优化研究

孙维1,汪开忠1,文光华2,唐萍2,刘慧3

(1.安徽省马鞍山市马鞍山钢铁股份有限公司技术中心
2.重庆大学 材料科学与工程学院, 重庆 400044
3.重庆大学 材料科学与工程学院,重庆 400030)

摘 要:由于异型坯形状复杂,在浇注耐候钢的过程中,铸坯表面质量较差,并经常发生粘结漏钢事故。通过实验室研究和工业性试验相结合的方法,根据异型坯连铸耐候钢的特点,分析了耐候钢异型坯表面质量差和浇注过程中发生粘结性漏钢的原因,提出了异型坯连铸耐候钢保护渣优化设计思路,重点研究了协调保护渣润滑和传热性能的影响因素。根据研究结果配制的异型坯连铸耐候钢专用保护渣,大生产应用结果表明,连浇炉数达到10炉以上,未发生粘结漏钢事故,耐候钢异型坯表面质量也有了明显提高。

关键词:连铸; 异型坯; 结晶器保护渣; 耐候钢

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号