Comparison of tribological properties of industrial low friction coatings

来源期刊:中国有色金属学报(英文版)2002年第1期

论文作者:王吉会 Hua Chen E. Wieers L.M. Stals J.P. Celis

文章页码:78 - 82

Key words:low friction coatings;fretting;relative humidity

Abstract: MX2 (M=Mo,W;X=S,Se) and DLC (a-C:H and WC/C) are the two kinds of typical low friction coatings widely used in industry.The friction and wear properties of these two kinds of coatings marked as MOVIC,MOST,MoSe2/Ni, WSe2,a-C: H and WC/C coatings were determined by fretting tests in ambient air of different humidity.The results show that the coefficient of friction of MX2 coatings increases when the relative humidity of air increases whereas the coefficient of friction DLC coatings decreases with the increasing of relative humidity.MOVIC and WSe2 coatings have a poor friction and wear resistance because of non-basal planes (100) and (101) parallel to the surface in the MOVIC coating, or the rough and porous surface of WSe2 coatings.Among these six coatings,MoSe2 /Ni and WC/C coatings have the highest wear resistance which seems to be unaffected by the relative humidity.

详情信息展示

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号