简介概要

Effect of near isothermal forging on the microstructure of Ti3Al/TC11 welding interface

来源期刊:Rare Metals2009年第5期

论文作者:LIU Yingying, YAO Zekun, and GUO Hongzhen College of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an , China

文章页码:471 - 477

摘    要:The as-forged Ti3Al-based alloy and TC11 titanium alloy were welded by electron beams in vacuum, and then they were processed using near isothermal forging and gradient heat treatment. The experimental results show that the near isothermal forging processing parameters have little effect on the phase constitution of the weld. The weld consists of Ti2AlNb, MoNb, Nb3Al, and TiAl3 phases as well as the two main phases of α and α2. However, the near isothermal forging processing parameters have significant effect on the shape, size, and volume fraction of α and α2 phases of the welding interface. The sizes of the α and α2 phases increase as the strain rate decreases. Because the distortion energy of the lattice and the volume fraction of the grains occurring in dynamic recrystallization increase with an increase in deformation, the sizes of the α and α2 phases of the welding interface decrease.

详情信息展示

Effect of near isothermal forging on the microstructure of Ti3Al/TC11 welding interface

LIU Yingying, YAO Zekun, and GUO Hongzhen College of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China

摘 要:The as-forged Ti3Al-based alloy and TC11 titanium alloy were welded by electron beams in vacuum, and then they were processed using near isothermal forging and gradient heat treatment. The experimental results show that the near isothermal forging processing parameters have little effect on the phase constitution of the weld. The weld consists of Ti2AlNb, MoNb, Nb3Al, and TiAl3 phases as well as the two main phases of α and α2. However, the near isothermal forging processing parameters have significant effect on the shape, size, and volume fraction of α and α2 phases of the welding interface. The sizes of the α and α2 phases increase as the strain rate decreases. Because the distortion energy of the lattice and the volume fraction of the grains occurring in dynamic recrystallization increase with an increase in deformation, the sizes of the α and α2 phases of the welding interface decrease.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号