摘    要:Monoclinic and hexagonal LaPO4:5 mol.%Eu3+ phosphors were synthesized with merely adjusting pH values of solutions by a hydrothermal method at the same synthesis temperature. The microstructure, morphology and photoluminescence of Eu3+-doped LaPO4, which were influenced by different preparation conditions, were characterized by X-ray diffraction(XRD), scanning electron microscopy(SEM), Fourier transform infrared spectroscopy(FT-IR), Raman spectroscopy and luminescence spectroscopy, respectively. The specimen showed monoclinic structure in strong acid solution, however, it changed into hexagonal structure in weak acid solution and strong alkali solution. The monoclinic LaPO4:Eu3+ showed the longest length to diameter ratio, which was attributed to the preferential growth of [-112]. The monoclinic specimen exhibited a slight red shift in infrared spectra, Raman band positions and charge transfer(CT) compared with hexagonal specimens. Moreover, the calculated results of grain sizes, lattice parameters, full width at half maximum in Raman patterns and emission integral intensity were in good agreement with analysis results. The monoclinic specimen showed the maximal absolute luminescence quantum yield(0.4) and the second lifetime τ2(0.52 ms), which was accordant with red-orange emission in CIE. The 5D07F1 occupied a dominate position in hexagonal specimens, which indicated that more Eu3+ in the hexagonal structure were occupied inversion center of symmetry sites.

详情信息展示

Vibrational and luminescent properties of LaPO4:Eu3+ with different preparation conditions

张忠举1,时婧2,王晓燕1,刘思达2,王昕2

1. College of Chemistry and Chemical Engineering,Ocean University of China2. Institute of Materials Science and Engineering,Ocean University of China

摘 要:Monoclinic and hexagonal LaPO4:5 mol.%Eu3+ phosphors were synthesized with merely adjusting pH values of solutions by a hydrothermal method at the same synthesis temperature. The microstructure, morphology and photoluminescence of Eu3+-doped LaPO4, which were influenced by different preparation conditions, were characterized by X-ray diffraction(XRD), scanning electron microscopy(SEM), Fourier transform infrared spectroscopy(FT-IR), Raman spectroscopy and luminescence spectroscopy, respectively. The specimen showed monoclinic structure in strong acid solution, however, it changed into hexagonal structure in weak acid solution and strong alkali solution. The monoclinic LaPO4:Eu3+ showed the longest length to diameter ratio, which was attributed to the preferential growth of [-112]. The monoclinic specimen exhibited a slight red shift in infrared spectra, Raman band positions and charge transfer(CT) compared with hexagonal specimens. Moreover, the calculated results of grain sizes, lattice parameters, full width at half maximum in Raman patterns and emission integral intensity were in good agreement with analysis results. The monoclinic specimen showed the maximal absolute luminescence quantum yield(0.4) and the second lifetime τ2(0.52 ms), which was accordant with red-orange emission in CIE. The 5D07F1 occupied a dominate position in hexagonal specimens, which indicated that more Eu3+ in the hexagonal structure were occupied inversion center of symmetry sites.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号