摘    要:A kind of far infrared radiation ceramics was prepared by using silicate minerals, calcium carbonate and silicon dioxide as main raw materials, and cerium nitrate as additive. The structure of the ceramics and far infrared radiation properties on the surface tension of water were characterized by X-ray diffraction, scanning electron microscopy, Fourier transform infrared spectroscopy and a tensiometer, respectively. It was showed that, after being sintered at 1160 °C, the solid solution was formed by CeO2 and Fe2O3, thus the crystal parameters(c/a axis ratio) and interplanar spacing of Fe2O3 increased. The addition of cerium was regarded to improve the far infrared radiation of ceramics, and the maximum emissivity value in the range of 5–20 μm was 0.94. The surface tension of water gradually decreased with increasing radiation time.

详情信息展示

Effect of far infrared radiation ceramics containing rare earth additives on surface tension of water

刘洁1,2,孟军平1,2,梁金生1,2,霍晓丽1,2

1. Institute of Power Source and Ecomaterials Science, Hebei University of Technology2. Key Laboratory of Special Functional Materials for Ecological Environment and Information (Hebei University of Technology), Ministry of Education

摘 要:A kind of far infrared radiation ceramics was prepared by using silicate minerals, calcium carbonate and silicon dioxide as main raw materials, and cerium nitrate as additive. The structure of the ceramics and far infrared radiation properties on the surface tension of water were characterized by X-ray diffraction, scanning electron microscopy, Fourier transform infrared spectroscopy and a tensiometer, respectively. It was showed that, after being sintered at 1160 °C, the solid solution was formed by CeO2 and Fe2O3, thus the crystal parameters(c/a axis ratio) and interplanar spacing of Fe2O3 increased. The addition of cerium was regarded to improve the far infrared radiation of ceramics, and the maximum emissivity value in the range of 5–20 μm was 0.94. The surface tension of water gradually decreased with increasing radiation time.

关键词:

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号