简介概要

Fabrication of TiO2 Nanotube Arrays by Rectified Alternating Current Anodization

来源期刊:JOURNAL OF MATERIALS SCIENCE TECHNOLOG2015年第1期

论文作者:Han Song Jing Shang Chen Suo

文章页码:23 - 29

摘    要:Anodization is a popular method of preparing TiO2 nanotube array films(TiNTs) by using direct current(DC)power as the driving voltage.In this study,three driving voltage modes,namely,the sine alternating current(sine) mode,the full-wave rectification of sine waves via four diodes(sine-4D,where D means diode) mode,and the DC mode,were used to prepare TiNTs by anodization.At 20 V,TiNTs were formed under sine-4D mode but only irregular porous TiO2 films were formed under DC mode.At 50 V,TiNTs formed under both the sine-4D and DC modes.No TiNTs formed in the sine mode anodization at either 20 or 50 V.Compared with the DC mode,the sine-4D mode required a lower oxidation voltage for TiNT formation,which suggests that sine-4D is an economical,convenient,and efficient driving voltage for TiNT preparation by anodization.The morphologies and structures of TiNT samples anodized at 50 V in the sine-4D and DC modes at different oxidation time(1,5,10,30,60,and 120 min) were analyzed.TiNT growth processes were similar between the studied modes.However,the growth rate of the films was faster under the sine-4D mode than the DC mode during the first 30 min of anodization.

详情信息展示

Fabrication of TiO2 Nanotube Arrays by Rectified Alternating Current Anodization

Han Song,Jing Shang,Chen Suo

State Key Joint Laboratory of Environmental Simulation and Pollution Control,College of Environmental Sciences and Engineering,Peking University

摘 要:Anodization is a popular method of preparing TiO2 nanotube array films(TiNTs) by using direct current(DC)power as the driving voltage.In this study,three driving voltage modes,namely,the sine alternating current(sine) mode,the full-wave rectification of sine waves via four diodes(sine-4D,where D means diode) mode,and the DC mode,were used to prepare TiNTs by anodization.At 20 V,TiNTs were formed under sine-4D mode but only irregular porous TiO2 films were formed under DC mode.At 50 V,TiNTs formed under both the sine-4D and DC modes.No TiNTs formed in the sine mode anodization at either 20 or 50 V.Compared with the DC mode,the sine-4D mode required a lower oxidation voltage for TiNT formation,which suggests that sine-4D is an economical,convenient,and efficient driving voltage for TiNT preparation by anodization.The morphologies and structures of TiNT samples anodized at 50 V in the sine-4D and DC modes at different oxidation time(1,5,10,30,60,and 120 min) were analyzed.TiNT growth processes were similar between the studied modes.However,the growth rate of the films was faster under the sine-4D mode than the DC mode during the first 30 min of anodization.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号