简介概要

Relationship among Mechanical Properties Anisotropy,Microstructure and Texture in AA 6111 Alloy Sheets

来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2016年第3期

论文作者:汪小锋 郭明星 CAO Lingyong PENG Xiangyang ZHANG Jishan ZHUANG Linzhong

文章页码:648 - 653

摘    要:We comparatively studied the mechanical properties anisotropy, microstructure and texture of the commercial and the new developed AA6111 alloys through tensile test, optical microscopy, and XRD analysis. The results show that the anisotropy of mechanical properties for the developed AA6111 alloy is lower than that of the commercial alloy. The developed alloy possesses higher r value, lower Δr value and more uniform microstructure, compared with the commercial AA6111 alloy, indicating that the deep drawability of the developed alloy has been improved significantly. The recrystallization textures of the two alloy sheets are also different. The recrystallization texture of the commercial alloy sheet mainly includes Cube and {114}<311> orientations, while the recrystallization texture of developed alloy sheet consists of Cube, Goss and R orientations. The relationships among the deep drawabilities, microstructure and texture were discussed thereafter.

详情信息展示

Relationship among Mechanical Properties Anisotropy,Microstructure and Texture in AA 6111 Alloy Sheets

汪小锋1,2,郭明星1,CAO Lingyong1,PENG Xiangyang1,ZHANG Jishan1,ZHUANG Linzhong1

1. State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing2. Faculty of Mechanical Engineering & Mechanics, Ningbo University

摘 要:We comparatively studied the mechanical properties anisotropy, microstructure and texture of the commercial and the new developed AA6111 alloys through tensile test, optical microscopy, and XRD analysis. The results show that the anisotropy of mechanical properties for the developed AA6111 alloy is lower than that of the commercial alloy. The developed alloy possesses higher r value, lower Δr value and more uniform microstructure, compared with the commercial AA6111 alloy, indicating that the deep drawability of the developed alloy has been improved significantly. The recrystallization textures of the two alloy sheets are also different. The recrystallization texture of the commercial alloy sheet mainly includes Cube and {114}<311> orientations, while the recrystallization texture of developed alloy sheet consists of Cube, Goss and R orientations. The relationships among the deep drawabilities, microstructure and texture were discussed thereafter.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号