简介概要

Micro bulging of thin T2 copper sheet by electromagnetic forming

来源期刊:中国有色金属学报(英文版)2011年第z2期

论文作者:ZHAO Qing-juan WANG Chun-ju YU Hai-ping GUO Bin SHAN De-bin LI Chun-feng

文章页码:461 - 464

Key words:sheet; micro-forming; micro bulging; electromagnetic forming

Abstract: Electromagnetic micro bulging experiments on T2 copper were achieved in order to find the effects that different voltages and depths of mold work on deformation characters. Laser scanning confocal microscope and contourgraph were used to study the effects of electromagnetic forming parameters such as voltage and die depth on material. Results show that width and depth of micro channel increase with the increases of voltage with a certain die depth, moreover, forming depth reaches the maximum at 7 500 V. And then rebound emerges and forming depth decreases. Forming depth and width of channel increase with the decease of die depth at a certain voltage; and forming depth reaches maximum at 0.5 mm of die depth. Therefore, rebound is weakened and the traces caused by bad exhaust disappears gradually, and surface roughness decreases simultaneously in electromagnetic bulging experiments.

详情信息展示

Micro bulging of thin T2 copper sheet by electromagnetic forming

ZHAO Qing-juan, WANG Chun-ju, YU Hai-ping, GUO Bin, SHAN De-bin, LI Chun-feng

(School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China)

Abstract:Electromagnetic micro bulging experiments on T2 copper were achieved in order to find the effects that different voltages and depths of mold work on deformation characters. Laser scanning confocal microscope and contourgraph were used to study the effects of electromagnetic forming parameters such as voltage and die depth on material. Results show that width and depth of micro channel increase with the increases of voltage with a certain die depth, moreover, forming depth reaches the maximum at 7 500 V. And then rebound emerges and forming depth decreases. Forming depth and width of channel increase with the decease of die depth at a certain voltage; and forming depth reaches maximum at 0.5 mm of die depth. Therefore, rebound is weakened and the traces caused by bad exhaust disappears gradually, and surface roughness decreases simultaneously in electromagnetic bulging experiments.

Key words:sheet; micro-forming; micro bulging; electromagnetic forming

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号