Synthesis and Structural Analysis of LDH-SO4-CO3 Whisker
来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2019年第5期
论文作者:吴健松 YANG Yifeng
文章页码:1085 - 1088
摘 要:High-quality LDH-SO4-CO3 whiskers were synthesized via liquid precipitation method using MgSO4·7 H2 O and Al2(SO4)3·18 H2O as precursors and Na2CO3-NaHCO3 buffer solution as precipitant. The influence of buffer solution concentration on the characteristics of the samples was investigated. The asgrown whiskers were characterized by X-ray diffraction, transmission electron microscopy, and BrunauerEmmett-Teller N2 specific surface area measurements. The results show that the buffer solution concentration has significant impact on whiskers with intercalated structure. The LDH-SO4-CO3 whiskers with well-defined geometry, distinct intercalated structure, decent quality, and excellent dispersing capability can be obtained under the following conditions: buffer solution volume ratio of 45%, reaction temperature of 83°C, and reaction time of 182 h. The obtained whiskers are well-crystallized and exhibit homogeneous morphology consisting of fiber bars.
吴健松1,YANG Yifeng2
1. School of Chemistry and Chemical Engineering, Lingnan Normal University2. School of Biological Science and Technology, Lingnan Normal University
摘 要:High-quality LDH-SO4-CO3 whiskers were synthesized via liquid precipitation method using MgSO4·7 H2 O and Al2(SO4)3·18 H2O as precursors and Na2CO3-NaHCO3 buffer solution as precipitant. The influence of buffer solution concentration on the characteristics of the samples was investigated. The asgrown whiskers were characterized by X-ray diffraction, transmission electron microscopy, and BrunauerEmmett-Teller N2 specific surface area measurements. The results show that the buffer solution concentration has significant impact on whiskers with intercalated structure. The LDH-SO4-CO3 whiskers with well-defined geometry, distinct intercalated structure, decent quality, and excellent dispersing capability can be obtained under the following conditions: buffer solution volume ratio of 45%, reaction temperature of 83°C, and reaction time of 182 h. The obtained whiskers are well-crystallized and exhibit homogeneous morphology consisting of fiber bars.
关键词: