Effect of coolant inhibitors on AZ91D
来源期刊:Rare Metals2004年第3期
论文作者:I.M. Baghni, WU Yinshun, ZHANG Wei, and LI Jiuqing ) Mechanical Engineering Department, Engineering College of Tajoura, Libya ) Corrosion and Protection Center, University of Science and Technology Beijing, Beijing , China
文章页码:255 - 259
摘 要:<正> The inhibition effects of sodium vanadate along with inorganic coolant inhibitors were examined on corrosion of AZ91D in ASTM D1384-80 corrosive water by polarization measurements. The galvanic corrosion of AZ91D coupled to 3003, 6063, and 356 Al alloys were also tested. An effective combination of inhibitors containing (but not limited to) sodium vanadate, silicate, and nitrate was proposed for inhibition of AZ91D and prevention of galvanic corrosion.
I.M. Baghni, WU Yinshun, ZHANG Wei, and LI Jiuqing 1) Mechanical Engineering Department, Engineering College of Tajoura, Libya 2) Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China
摘 要:<正> The inhibition effects of sodium vanadate along with inorganic coolant inhibitors were examined on corrosion of AZ91D in ASTM D1384-80 corrosive water by polarization measurements. The galvanic corrosion of AZ91D coupled to 3003, 6063, and 356 Al alloys were also tested. An effective combination of inhibitors containing (but not limited to) sodium vanadate, silicate, and nitrate was proposed for inhibition of AZ91D and prevention of galvanic corrosion.
关键词: