Hydrothermal synthesis and luminescence properties of YW2O6(OH)3:Tb3+ green phosphors
来源期刊:Journal of Rare Earths2011年第7期
论文作者:张大凤 蒲锡鹏 仪修杰 邵鑫 钱先华 李梅静 吴淑通
文章页码:628 - 631
摘 要:YW2O6(OH)3:Tb3+ green phosphors were synthesized at different pH values via a facile hydrothermal method. The structure and optical properties of as-synthesized samples were studied by X-ray diffractometer (XRD), scanning electron microscopy (SEM), photolumi-nescence spectra and luminescence decay curve. The results showed that pure monoclinic YW2O6(OH)3:Tb3+ green phosphors could be ob-tained at pH 2-5. Uniform spherical micro-phosphors of 5 μm in diameter with narrow size distribution could be prepared at pH 5. pH value had dramatic influence on morphologies, which could be ascribed to the various spatial configurations of different poly-tungstates existing at different pH values. The emission spectra under 261 nm excitation exhibited dominant green emission at 546 nm. The green emission inten-sity reached the maximum value at pH 5 due to the high packing density of the obtained phosphor.
张大凤,蒲锡鹏,仪修杰,邵鑫,钱先华,李梅静,吴淑通
School of Materials Science and Engineering, Liaocheng University
摘 要:YW2O6(OH)3:Tb3+ green phosphors were synthesized at different pH values via a facile hydrothermal method. The structure and optical properties of as-synthesized samples were studied by X-ray diffractometer (XRD), scanning electron microscopy (SEM), photolumi-nescence spectra and luminescence decay curve. The results showed that pure monoclinic YW2O6(OH)3:Tb3+ green phosphors could be ob-tained at pH 2-5. Uniform spherical micro-phosphors of 5 μm in diameter with narrow size distribution could be prepared at pH 5. pH value had dramatic influence on morphologies, which could be ascribed to the various spatial configurations of different poly-tungstates existing at different pH values. The emission spectra under 261 nm excitation exhibited dominant green emission at 546 nm. The green emission inten-sity reached the maximum value at pH 5 due to the high packing density of the obtained phosphor.
关键词: