共搜索到122041条信息,每页显示10条信息,共12205页。用时:0小时0分1秒177毫秒
Trans. Nonferrous Met. Soc. China 22(2012) s645-s649 Effect of bonding interface on delamination behavior of drawn Cu/Al bar clad material Sangmok LEE1, Min-Geun LEE2, Sang-Pill LEE3, Geun-Ahn LEE1..., Dong-Eui University, Busan 614-714, Korea; 3. Department of Mechanical Engineering, Dong-Eui University, Busan 614-714, Korea Received 21 May 2012; accepted 27 September 2012 Abstract: Cu/Al bar clad......
......
......
Multilayer Clad Plate of Stainless Steel/Aluminum/Aluminum Alloy袁家伟,庞玉华School of Metallurgy Engineering, Xi’an University of Architecture & Technology摘 要:The 3, 5, 20 layer clad plate from austenitic stainless steel, pure aluminum and aluminum alloy sheets were fabricated in different ways. The stretch and interface properties were measured. The result......
High-temperature deformation behavior of titanium clad steel plateShang-Wu Zeng1,2,Ai-Min Zhao1,2,Hai-Tao Jiang1,Xiao-Qian Yan1,Ji-Xiong Liu3,Xiao-Ge Duan11. Engineering Research Institute..." name="ChDivSummary">In this paper, the single-pass hot compression experiment of titanium clad steel plate was carried out by Gleeble-3500 thermal mechanics simulation test machine,and the effect......
steel/Ti clad materials using the roll bonding method. PARK et al [9] conducted finite element analysis on tube extrusion of Al/Cu clad composite material by hydrostatic extrusion method, and examined... bar clad materials in terms of post aging time to have a proper bonding strength. In the present study, the billet of duo-cast Al 3003/Al 4004 clad materials was in circle shape, which was composed......
Electrochemical Behavior of Steel Bar in Electrolytes:Influence of pH Value and Cations濮琦College of Mechanics and Materials,Hohai University摘 要:Steel bar... of free corrosion potential and electrochemical impedance spectra (EIS) were used to evaluate the influence of cations on the depassivation of the steel bar in electrolytes. The experimental results......
Effect of Interlayers on Microstructure and Properties of 2205/Q235B Duplex Stainless Steel Clad PlateFengqiang Xiao1,2,3,Dongpo Wang1,2,Wenbin Hu1,Lei Cui1,2,Zhiming Gao1,Lanju Zhou41. School... on the bonding interface structures and the shear strengths of the clad steel plates were studied.The results showed that 2205 duplex stainless steel and the three interlayers produced a large amount......
; Degradation of bond between steel bar and freeze...; Abstract: The effect of electrochemical chloride extraction (ECE) on bond strength between steel bar and freeze-thaw concrete contaminated......
Effect of annealing on two different niobium-clad stainless steel PEMFC bipolar plate materials Sung-Tae HONG1, Dae-Wook KIM2, Yong-Joo YOU2, K. Scott WEIL3 1. School of Mechanical... that it can be subsequently blanked, stamped and dimpled in forming the final plate component. Two roll bonded materials, niobium clad 340L stainless steel (Nb/340L SS) and niobium clad 434 stainless......