共搜索到11532条信息,每页显示10条信息,共1154页。用时:0小时0分1秒578毫秒
Article ID: 1003-6326(2005)05-1085-04 Maximum solid solubility of transition metals in vanadium solvent ZHANG Jin-long(张金龙)1, FANG Shou-shi(方守狮)1, ZHOU Zi-qiang(周自强)1, LIN Gen-wen(林根文)1, GE Jian..., University of Windsor, Windsor, Ont., Canada N9B 3P4) Abstract: Maximum solid solubility (Cmax) of different transition metals in metal solvent can be described by a semi-empirical equation using function......
......
......
......
Solid Solubility and Age Hardening of Rapidly Solidified Al-Er Alloys宁远涛,戴红摘 要:<正> The metastable extension of solid solubility and age hardening... spinning techniques,respectively.The cooling rate wasabout 106~107 K/s.The metastable extended solid solubility of Er in Al evaluated by measurements of lat-tice parameters of rapidly solidified alloys......
......
in copper Solid solubility extensions have been achieved in many alloy systems by mechanical alloying. Solid solubility levels have been generally determined from changes in the lattice parameter values... Conclusions Solid solubility extensions have been achieved in C/Cu alloy systems by mechanical alloying. The lattice parameter increases with milling time, and reaches a maximum value at approximately 24......
Solid solubility extension and microstructure evolution of cast zirconium yttrium alloyJia-Qing Peng1,2,Yang Chen1,Guo-Qing Yan1,Ming Wu1,Li-Jun Wang1,Jing-She Li21. Division of Rare Metals...="ChDivSummary">Yttrium addition can improve the oxidation resistance,mitigate hydrogen embrittlement and thus enhance the mechanical properties of the zirconium alloy.To study solid solubility extension......
......
果表明:施加超声外场铸锭的凝固组织与未施加超声外场铸锭的相比明显细化,铸锭中形成大量细小,均匀的等轴晶组织,溶质元素在晶内的固溶度增大;Zn,Mg和Cu的晶内相对溶质固溶度分别提高17.468%,49.549%和21.849%.关键词:7050铝合金;超声;显微组织;固溶度Effects of ultrasonic on microstructures and solid solubility... 7050; ultrasound; microstructure; solid solubility......