Wrinkling behavior of magnesium alloy tube in warm hydroforming TANG Ze-jun(汤泽军), LIU Gang(刘 钢), HE Zhu-bin(何祝斌), YUAN Shi-jian(苑世剑) School of Materials Science and Engineering, Harbin Institute... occur and affect the forming results. Wrinkling behavior of an AZ31B magnesium alloy tube was experimentally investigated with different loading paths at different temperatures. Features of wrinkles......
ZK60 alloy ingot (the chemical composition (mass fraction, %): Zn 5.6, Zr 0.54, Fe≤0.003, Ni≤0.002, Mg balance) with a diameter of d129 mm was used in the experiments. The specimens were taken from... Effects of heat-treatment on microstructure of wrought magnesium alloy ZK60 MA Yan-long(麻彦龙)1, 2, PAN Fu-sheng(潘复生)2, ZUO Ru-lin(左汝林)2, ZHANG Jin(张 津)1, YANG Ming-bo(杨明波)1 1. College......
Article ID: 1003-6326(2005)03-0565-06 Amorphous coatings deposited on aluminum alloy by plasma electrolytic oxidation GUAN Yong-jun(关永军), XIA Yuan(夏 原) (Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, China) Abstract: Amorphous [Al-Si-O] coatings were deposited on aluminum alloy by plasma electrolytic oxidation(PEO). The process parameters......
of the structural aircraft parts. 2 EXPERIMENTAL The Al alloy assessed in this investigation was AA 7010-T7651 with a chemical composition of Zn 6.30, Mg 2.34, Cu 1.75, Zr 0.12, Fe 0.05, Si 0.04, Ti... Article ID: 1003-6326(2005)06-1258-06 Variations of properties across plate thickness for Al alloy 7010 M. Salazar-Guapuriche1, 2, Y. Y. Zhao2, A. Pitman3, A. Greene3 (1. Materials......
......
......
......
......
......