共搜索到1153条信息,每页显示10条信息,共116页。用时:0小时0分0秒385毫秒
through chemical vapor deposition (CVD) or wet chemistry. WANG et al [46] deposited a graphene/MWCNT foam via CVD and subsequently dip-coated it with RuO2 suspension to form a RuO2/graphene/CNT hybrid......
REVIEW J. Cent. South Univ. (2019) 26: 1021-1041 DOI: https://doi.org/10.1007/s11771-019-4068-9 A review on application of nanofluid in various types of heat pipes Mohammad Alhuyi NAZARI1, Mohammad H. AHMADI2, Milad SADEGHZADEH1,Mohammad Behshad SHAFII3, Marjan GOODARZI4 1. Department of Renewable......
. In a typical experiment, a homogeneous suspension comprised of catalyst, hydroxypropyl cellulose, and distilled water was obtained by constantly stirring at 60 °C followed by the injection of the slurry......