共搜索到6859条信息,每页显示10条信息,共686页。用时:0小时0分0秒459毫秒
......
Corrosion behavior of Mg and Mg-Zn alloys in simulated body fluid GAO Jia-cheng(高家诚)1, 2, WU Sha(伍 沙)1, QIAO Li-ying(乔丽英)1, 2, WANG Yong(王 勇)1 1. College of Materials Science and Engineering...: The corrosion behavior of Mg and Mg-Zn in simulated body fluid was studied. The mass loss of pure Mg, Mg-Zn-Zr and Mg-Zn-Zr-Y in simulated body fluid was measured using photovoltaic scale meter. Corrosion......
......
......
......
pH value in simulated occluded corrosion cell for magnesium alloys ZENG Rong-chang(曾荣昌)1, CHEN Jun(陈君)1, KE Wei(柯伟)2, Han En-hou(韩恩厚)2, W. Dietzel3 1. School of Materials Science and Engineering, Chongqing Institute of Technology, Chongqing 400050, China; 2. Environmental Corrosion Center, Institute of Metals Research, Chinese Academy of Sciences, Shenyang 110016, China; 3. GKSS Research......
Effects of rotating electromagnetic on flow corrosion of copper in seawaterLI Ji-nan, ZHANG Peng, GUO Bin(School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China)Abstract:The flow corrosion of copper in seawater was investigated with the rotating electromagnetic corrosion experimental bench for 12 d. Scanning electron microscopy equipped with EDAX and X......
Corrosion properties of plastically deformed AZ80 magnesium alloy ZHANG Zhi-min(张治民),XU Hong-yan(徐宏妍), LI Bao-cheng(李保成) School of Materials Science and Engineering, North University of China...%, 83%, 87% and 90%, respectively. The corrosion properties of different deformed AZ80 samples were studied by galvanic test in 3.5% NaCl solution. The results show that plastic deformation could......
An evaluation analysis method for corrosion morphology characterization based on Gaussian filter ZHANG Peng (张 鹏)1, GUO Bin (郭 斌)2, CHENG Shu-kang (程树康)3 1. School of Materials Science...; Abstract: The corrosion process of copper in thermal flow system was investigated......
J. Cent. South Univ. (2020) 27: 2530-2537 DOI: https://doi.org/10.1007/s11771-020-4478-8 Microstructure and hot corrosion resistance of Si-Al-Y coated TiAl alloy LI Yong-quan(李涌泉)1, 2, XIE Fa-qin(谢... the requirements in hot corrosion environment, Si-Al-Y coatings were fabricated by pack cementation process at 1050℃ for 4 h. Corrosion behaviors of the TiAl alloy with and without Si-Al-Y coatings are compared......