共搜索到1772条信息,每页显示10条信息,共178页。用时:0小时0分0秒234毫秒
of polycrystalline YAG:Ce3+ phosphors (particle size: 30-50 μm) were measured by a fluorescence spectrophotometer (F-4500, Hitachi, Tokyo, Japan, wavelength range: 310-650 nm, scan speed: 1 200 nm/min... Crystallization, morphology and luminescent properties of YAG:Ce3+ phosphor powder prepared by polyacrylamide gel method LIU Chun-jia(刘春佳), YU Rui-min(于瑞敏), XU Zhi-wei(许志伟), CAI Jing(蔡 靖),YAN Xing......
Thermal residual stress of polycrystalline diamond compacts CHEN Feng(陈 枫)1, XU Gen(徐 根)2, MA Chun-de(马春德)1, XU Guo-ping(徐国平)3 1. Testing Center, Central South University, Changsha...; Abstract: Thermal residual stresses in polycrystalline diamond compact (PDC) cutter arising from the difference in thermal expansion between the polycrystalline diamond (PCD......
Institute, Beijing 100072, China) Abstract:Neodymium doped-yttrium aluminum garnet (Nd: YAG) transparent polycrystalline ceramics already become substitutes of single crystals because they are provided with easy fabrication, low cost, large size, highly doped concentration, high heat conductivity, mass fabrication, multi-layers and multi-functions. The Nd: YAG precursor powders with loosely dispersed......
添加ZrO2对YAG纤维物相和形貌的影响谭宏斌陕西理工学院材料学院摘 要:以氯化铝,金属铝粉,氧化钇,氧氯化锆,醋酸为原料,采用溶胶-凝胶法制备了钇铝石榴石(YAG)纤维,并研究添加ZrO2对YAG纤维的物相和形貌的影响.结果表明,添加ZrO2的YAG纤维物相仍为钇铝石榴石相,纤维表面光滑且直径均匀;ZrO2可作为YAG纤维的增韧相.关键词:YAG纤维;物相;形貌;ZrO2增韧;......
PRESS FORMABILITY OF YAG LASER WELDED TRIP STEEL SHEETS A.Nagasaka1 (1.Department of Mechanical Engineering, Nagano National College of Technology, 716 Tokuma, Nagano 381-8550, Japan) Abstract:The effects of YAG laser welding conditions on mechanical properties and pressformability (bendability, stretch-formability and deep drawability) of high-strengthtransformation-induced plasticity-aided......
......
掺杂YAG闪烁晶体研究进展牛雪姣1,2,徐家跃1,21. 上海应用技术学院材料科学与工程学院2. 上海应用技术学院晶体生长研究所摘 要:总结了不同离子掺杂YAG晶体的生长,闪烁特性和Ce∶YAG晶体的发光机理.Yb∶YAG晶体具有非常短的衰减时间(0.98ns),但光产额只有约1190phot/MeV.Ce∶YAG晶体的衰减时间为88ns,光产额可达26000phot/MeV,它具有优良的综合性能,已应用于闪烁探测器和大规模集成电路检测.Gd或Gd/Ga等稀土离子与Ce共掺可进一步提高YAG晶体的闪烁性能,最高光产额达44000phot/MeV,衰减时间为56.9ns.关键词:YAG晶体;掺杂;闪烁性能;发光机理;......
白光LED用Ce∶YAG微晶玻璃的研究进展张志敏1,向卫东1,钟家松2,刘炳峰1,梁晓娟1,陈兆平1,赵斌宇21. 温州大学化学与材料工程学院2. 同济大学材料科学与工程学院摘 要:Ce∶YAG微晶玻璃是一种可替代荧光粉用于白光LED的新型高性能荧光材料.综述了YAG微晶玻璃的制备方法,性能影响因素,发光机理,指出了Ce∶YAG微晶玻璃应用于白光LED的优势,并展望了白光LED用YAG微晶玻璃的发展趋势.关键词:钇铝石榴石(YAG);微晶玻璃;白光LED;......
-gel based ceramic-ceramic 0-3 composite[J]. Surface and Coatings Technology, 1995, 76-77: 113-118. [15] Towata A, Hwang H J, Yasuoka M. Preparation of polycrystalline YAG/alumina composite fibers...文章编号: -1004-0609(2005)04-0524 -07 YAG引入方式对碳化硅陶瓷烧结特性,力学性能及结构的影响 郭兴忠1, 杨 辉1, 王建武1, 高黎华2, 李祥云2 (1. 浙江大学 纳米科学与技术中心, 杭州 310027;2. 浙江东新密封材料有限公司, 乐清 325604) - 摘 要: 采用溶胶-凝胶法和机械共混法分别引入烧结助剂YAG(Y3Al5O12)和......
Nd∶YAG激光透明陶瓷的研究进展张乐1,2,周天元3,陈浩1,杨浩1,张其土3,宋波2,汪正平21. 江苏师范大学物理与电子工程学院江苏省先进激光材料与器件重点实验室2. 佐治亚理工学院材料科学与工程学院3. 南京工业大学材料科学与工程学院摘 要:作为新一代固体激光增益介质,Nd∶YAG透明陶瓷以容易制造,成本低,易于实现大尺寸生产等优势,正逐步取代单晶和玻璃材料,应用前景十分广阔.从Nd∶YAG透明陶瓷光学质量的提升,激光输出特性以及实现Nd∶YAG透明陶瓷高功率激光输出3个方面,分别回顾并总结了我国,日本,美国,欧洲和俄罗斯关于Nd∶YAG激光透明陶瓷的研究进展,并概述了我国及日本关于复合结构及共掺杂Nd∶YAG透明陶瓷的发展情况.最后总结并展望了当前Nd∶YAG激光透明陶瓷的发展趋势和存在的主......