共搜索到292条信息,每页显示10条信息,共30页。用时:0小时0分0秒249毫秒
J. Cent. South Univ. (2020) 27: 2792 DOI: https://doi.org/10.1007/s11771-020-4499-3 Retraction note to "Development and characterization of hot dip aluminide coated stainless steel 316L" (J. Cent... to correspondence about this retraction. [1] MUKHTAR S, ASGHAR W, BUTT Z, et al. Development and characterization of hot dip aluminide coated stainless steel 316L [J]. J Cent South Univ, 2018, 25(11): 2578–2588......
......
Identification of Phases in Aluminide Coatings by Means of Interference Layer Metallography吴维叟摘 要:<正> Interference layer metallography was usedto identify the phases present in the aluminidecoating on superalloy IN738LC. They are: twointermetallic aluminides NiAl and Ni3Al, y-solidsolution and a Cr-rich solid solution, twosulphides M23C6 and MC......
Oxidation Performance and Interdiffusion Behavior of a Pt-Modified Aluminide Coating with Pre-deposition of NiHe Liu1,2,Shuai Li1,2,Cheng-Yang Jiang3,Chun-Tang Yu1,2,Ze-Bin Bao1,Sheng-Long Zhu1,Fu-Hui Wang31. Institute of Metal Research,Chinese Academy of Sciences2. School of Materials Science and Engineering,University of Science and Technology of China3. Shenyang National Laboratory......
Improving cyclic oxidation resistance of Ni3Al-based single crystal superalloy with low-diffusion platinum-modified aluminide coatingH.Liu1,2,M.M.Xu1,2,S.Li1,2,Z.B.Bao1,S.L.Zhu1,F.H.Wang31. Institute of Metal Research, Chinese Academy of Sciences2. School of Materials Science and Engineering, University of Science and Technology of China3. Shenyang National Laboratory for Materials Science......
......
or the volume fraction of γ phase). Key words: titanium aluminide alloy; heat treatment; microstructure evolution; grain growth TiAl基合金由于具有高比强度,优异的高温强度和优良的抗氧化性能[1-8],在汽车及航空航天领域有着广泛的应用前景.TiAl基合金室温脆性大而且热加工变形...]. The Chinese Journal of Nonferrous Metals, 2014, 24(5): 1241-1250. [6] ABDALLAH Z, WHITTAKER M T, BACHE M R. High temperature creep behaviour in the γ titanium aluminide Ti-45Al-2Mn-2Nb[J......
behavior of microcrystalline aluminide coatings by electro-pulse deposition MA Jing1, 2, HE Ye-dong2, WANG Jun1, SUN Bao-de1 (1. State Key Laboratory of Metal Matrix Composites, Shanghai Jiao Tong... Ar to protect samples from oxidation. The coatings are metallurgically bonded to the substrate without obvious interface. The samples with aluminide coatings for oxidation were put in air at 600......
Effect of Substrate Characteristics on Interdiffusion Coefficients of Ni and Al Atoms in β-NiAl Phase of Aluminide CoatingsHua WEI, Xiaofeng SUN, Qi ZHENG, Guichen HOU, Hengrong GUAN and Zhuangqi HUInstitute of Metal Research, The Chinese Academy of Sciences, Shenyang 110016, China摘 要:<正> Interdiffusion coefficients at 950℃ and 1050℃function......
IN738合金上铂铝涂层的高温氧化 王文1,刘刚1,牛焱1,吴维1 (1.中国科学院金属研究所金属腐蚀与防护国家重点实验室沈阳 110016) 摘要:研究了IN738镍基高温合金的铂改性渗铝涂层在1100℃空气中的氧化行为.铂的存在,通过阻止合金元素穿过Al2O3膜向外扩散,改善AlO3膜与基体的结合力,抑制γ′-Ni3Al相的形成,推迟涂层的高温退化,同时讨论铂的作用机制. 关键词:铂铝化物涂层高温氧化; platinum; aluminide coating; oxidationCu- Al; [全文内容正在添加中] ......