共搜索到4017条信息,每页显示10条信息,共402页。用时:0小时0分2秒406毫秒
Removal of vanadium from ammonium molybdate solution by ion exchange LI Qing-gang(李青刚)1, 2, ZHANG Qi-xiu(张启修)2, ZENG Li(曾 理)2, XIAO Lian-sheng(肖连生)1, 2, YANG Ya-nan(杨亚男)2 1. State Key Laboratory...; Abstract: The separation techniques of vanadium and molybdenum were summarized, and a new method of removal V(Ⅴ) from Mo(Ⅵ) by adsorption with chelate resin was presented. Nine......
excellent physicochemical properties [1,2]. Vanadium and its compounds originate mostly from primary sources such as ore feedstock and concentrates [3], secondary sources such as metallurgical slags.... [17] FU Zi-bi. Development process and trends of vanadium extraction from vanadium-titanium magnetite ore [J]. China Nonferrous Metallurgy, 2011, 40(6): 29-33. (in Chinese) [18] CHEN Hou-sheng......
A method for recovery of iron, titanium, and vanadium from vanadium-bearing titanomagnetiteYi-min Zhang1,2,3,Li-na Wang2,3,De-sheng Chen2,3,Wei-jing Wang2,3,Ya-hui Liu2,3,Hong-xin Zhao2,3,Tao Qi2,31... of Process Engineering, Chinese Academy of Sciences摘 要:An innovative method for recovering valuable elements from vanadium-bearing titanomagnetite is proposed......
......
Metalizing reduction and magnetic separation of vanadium titano-magnetite based on hot briquettingShuang-yin Chen,Man-sheng ChuSchool of Materials and Metallurgy, Northeastern University摘 要:To achieve high efficiency utilization of Panzhihua vanadium titano-magnetite, a new process of metalizing reduction and magnetic separation based on hot briquetting......
ore is one of the main ore feedstocks for the recovery of vanadium in China and significant quantities of vanadium bearing slag (V-slag) containing 12%-20% V2O5 is generated as byproduct from the iron...Trans. Nonferrous Met. Soc. China 24(2014) 2687-2694 Extraction of vanadium from molten vanadium bearing slag by oxidation with pure oxygen in the presence of CaO Wen-chen SONG1,2, Hong LI1,2, Fu......
Characteristics of graphite felt electrode electrochemically oxidized for vanadium redox battery application LI Xiao-gang(李晓刚)1, HUANG Ke-long(黄可龙)1, LIU Su-qin(刘素琴)1, TAN Ning(谭 宁)1, CHEN Li... as electrode for vanadium redox battery was investigated with FT-IR, SEM, XPS, BET, cyclic voltammetry and testing VRB system, respectively. The results show that the molar ratio of O to C increases from 0.085......
and dissociation characteristics of vanadium titano-magnetite(VTM) ore were investigated using scanning electron microscopy(SEM), nitrogen absorption measurements, particle size distribution measurements...Influence of microwave treatment on grinding and dissociation characteristics of vanadium titano-magnetiteJun-peng Wang1,Tao Jiang1,2,Ya-jing Liu1,Xiang-xin Xue1,21. School of Metallurgy......
Vanadium extraction and dephosphorization from V-bearing hot metal with fluxes containing CaOWANG Yan-nan(王艳南)1, 2, SONG Wen-chen(宋文臣)1, 2, LI Hong(李宏)1, 2(1. State Key Laboratory of Advanced...)Abstract:Extracting vanadium and removing phosphorus simultaneously by adding CaO containing materials to V-bearing hot metal were investigated under the condition of simulating the process of vanadium......
......