共搜索到20356条信息,每页显示10条信息,共2036页。用时:0小时0分0秒765毫秒
Subtransus deformation mechanisms of TC11 titanium alloy with lamellar structure SONG Hong-wu(宋鸿武), ZHANG Shi-hong(张士宏), CHENG Ming(程 明) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China Received 13 October 2009; accepted 23 August 2010 Abstract: Isothermal compression tests are applied to study the deformation mechanisms of TC11 titanium alloy with lamellar......
Plasma surface alloying of titanium alloy for enhancing burn-resistant property ZHANG Ping-ze(张平则) 1, XU Zhong(徐 重) 1,2, ZHANG Gao-hui(张高会) 2, HE Zhi-yong(贺志勇) 2,YAO Zheng-jun(姚正军) 1 1.School... 030024,China Received 28 July 2006; accepted 15 September 2006 Abstract: Conventional titanium alloy may be ignited and burnt under high temperature, high pressure and high gas flow velocity condition......
Effects of thermohydrogen treatment on microstructures
of α+β and β titanium alloy as-cast
ZHAO Yong-qing(赵永庆), CAO Xing-min(曹兴民), XI Zheng-ping(奚正平)
Northwest Institute for Nonferrous Metal...: titanium alloy; thermohydrogen treatment; microstructure
Influence of deformation parameters on microstructure and mechanical properties of TA15 titanium alloy
ZHU Jing-chuan(朱景川), WANG Yang(王洋), LIU Yong(刘勇),
LAI Zhong-hong(来忠红), ZHAN Jia-jun(占家军... on the microstructure and mechanical properties of TA15 titanium alloy was studied. The volume fraction, size and aspect ratio of primary α phase in deformed TA15 titanium alloy were quantitatively......Influence of deformation parameters on microstructure and mechanical properties of TA15 titanium alloy
AI导读
来源: 《中国有色金属学报(英文版)2007年增刊第1期》——朱景川 王洋 刘勇 来忠红 占家军
Effect of titanium addition on fracture toughness behavior of ZL108 alloy WENG Yong-gang(翁永刚), LI Zi-jing(李姿景), LIU Zhi-yong(刘志勇), LIU Wen-cai(刘文才), WANG Ming-xing(王明星), SONG Tian-fu(宋天福) Key... titanium alloying methods were applied to ZL108 alloy for preparing specimens containing titanium. The specimens were tested on the MTS 810 material test system for studying their behavior of the plane......
) in titanium alloy TC11 at high temperature and the influence of oxygen solution layer on performances of substrate were characterized with the help of apparatus, such as TGA,SEM/EDAX, XRD, EPMA, Micro-hardness...An Oxygen-Permeation Treatment for Hardening Titanium Alloys WANG Mao-cai1,WEI Zheng2,MA Hong-yan1,XIN Gong-chun2 (1.State Key Laboratory for Corrosion and Protection, Institute of Metal Research......
Effect of size and distribution of titanium carbide on microstructure and mechanical properties of Ti-25V-15Cr-2Al-0.2C-0.2Si alloy LEI Li-ming(雷力明)1, HUANG Xu(黄 旭)1, WANG Bao(王 宝)1... DE24 8BJ, U.K.) Abstract: The effect of size and distribution of titanium carbide on the microstructure and mechanical properties of non-burning β titanium alloy Ti-25V-15Cr-2Al-0.2C-0.2Si (mass......
Effect of YF3 on weld microstructure and performance of titanium alloy TC4 in TIG weldingYANG Chun-li(杨春利), LIN San-bao(林三宝), ZHANG Qing-tao(张清涛)(State Key Laboratory of Advanced Welding Production Technology,Harbin Institute of Technology, Harbin 150001, China)Abstract:The effect of additive YF3 on weld microstructure and mechanical performance of titanium alloy TC4 in Activating Tungsten Inert......
......
Article ID: 1003-6326(2005)05-1081-04 Double-sided gas tungsten arc welding process on TC4 titanium alloy GAO Hong-ming(高洪明), BAI Yan(白 岩), YANG Tian-dong(杨天东) (State Key Laboratory of Advanced Welding Production Technology, Harbin Institute of Technology, Harbin 150001, China) Abstract: TC4 titanium alloy was welded by double-sided gas tungsten arc welding(GTAW) process in comparison......