共搜索到2527条信息,每页显示10条信息,共253页。用时:0小时0分0秒359毫秒
......
, China; 4. Xi’an University of Science and Technology, College of Safety Science and Engineering, Xi’an 710054, China) Abstract: The circular thin plate specimens of different porosity were made by the method of controlling sand sizes. RSM-SY7 automatic ultrasonic measuring instrument with foundation piles and more cross-holes was used to measure and mark the values of porosity. Permeability test......
......
with a series of experiments including casting thin slice, SEM, the techniques of physical properties and so on. And a simulation equation corresponding to porosity was established according to the feature of diagenetic evolution and the generalized geologic effect. By comparing the route of porosity evolution of Chang 6 sandstone reservoir in Jiyuan Oilfield and Huaqing Oilfield, the difference......
; 文章编号:1672-7207(2011)11-3438-09 Microstructure characteristics and quantitative analysis on porosity evolution of ultra-low sandstone reservoir WU Xiao-bin1, 2... of Geology, Northwest University, Xi’an 710069, China) Abstract: The average porosity of sandstone reservoir in Jiyuan area of Ordos basins is 11.68%, average permeability is 0.58×10-3μm2, belonging......
Trans. Nonferrous Met. Soc. China 26(2016) 835-841 Effect of ore size and heap porosity on capillary process inside leaching heap Sheng-hua YIN1, Lei-ming WANG1, Xun CHEN1, Ai-xiang WU2 1. Key... to the dual-porosity structure. Capillary rise is responsible for the mineral dissolution in fine particle zones and interior coarse rock. The effect of particle size and heap porosity on the capillary......
. Porosity control and compressive strength of porous zirconia prepared by freeze casting[J]. The Chinese Journal of Nonferrous Metals, 2021, 31(8): 2059-2068. DOI: 10.11817/j.ysxb.1004.0609.2021-41030 多孔氧化锆... 不同固相含量制备多孔氧化锆陶瓷的显微组织 Fig. 5 Microstructures of porous zirconia prepared with different solid loading 表2 试样的烧结收缩率,孔隙率及抗压强度 Table 2 Sintering shrinkage, porosity and compressive......
Powder Size Influence on Tensile Properties and Porosity for PM Ti2AlNb Alloy Prepared by Hot Isostatic PressingZheng-Guan Lu1,2,Jie Wu1,Lei Xu1,Rui Yang11. Institute of Metal Research , Chinese Academy of Sciences2. School of Materials Science and Engineering , University of Science and Technology of China摘 要:Pre-alloyed powder of Ti2AlNb alloy......
geometry, porosity, microstructure and mechanical properties of the stitch welded seams were investigated by digital microscope, optical microscope, scanning electron microscope and universal tensile... nozzle. Porosity formation could be suppressed with the gap between plate and skeleton less than 0.1 mm, while the existing porosity can be reduced with remelting. The maximum shear strength of stitch......
porosity 5.1%. With the addition of 5%(mass fraction) CNTs, the density of the composite block is elevated to 1.84 g/cm3, and its open porosity is reduced to 3.5%. The flexural strength of composite block...; flexural strength; density; open porosity  ......