共搜索到29010条信息,每页显示10条信息,共2901页。用时:0小时0分0秒484毫秒
Effect of annealing temperature on the microstructure and optoelectrical properties of ZnO thin films and their application in self-powered accelerometersXiao-zhou Zhang,Yan-ping Xia,Xing Liu,Yi-ming... the device with an AZO/ZnO/PMMA/stainless steel configuration. In addition, the annealing temperature affected the open-circuit voltage of the NGs; the output voltage reached 3.81 V when the annealing......
decreased gradually with raising the annealing temperature. Probable causes of the generation of the residual stress and the changes in mechanical properties and fracture mode due to the irradiation...Ion Beam Surface Modification of Y-TZP and Effects of Subsequent Annealing M.Ishihara1,T. Sakuma2,K.Sawa1,S.Baba1,S.Harjo2,Y. Motohashi2,T. Shibata1 (1.Oarai Research Establishment, JAERI, Oarai......
Influence of annealing temperature on electrochemical properties of rapidly quenched LPC(NiAlMn)4.25Co0.75 hydrogen storage alloy electrodes ZHENG Qun(郑 群), CHEN Yun-gui(陈云贵), WANG Jin-guo(王金国), TAO Ming-da(陶明大), TANG Ding-xiang(唐定骧), TU Ming-jing(涂铭旌) (Department of Metallic Materials, Sichuan University, Chengdu 610065, China) Abstract: The influence of annealing temperature......
工艺参数对800MPa热镀锌双相钢组织性能的影响金光灿1,赵征志2,徐刚2,赵爱民2,刘光明3(1.北京市北京科技大学 冶金与生态工程学院2.北京科技大学 冶金工程研究院,北京 1000833.首钢技术研究院,北京 100039)摘 要:在实验室试制了低Si的C-Mn-Cr-Mo系的800 MPa级冷轧热镀锌双相钢,研究了卷取温度,退火温度,退火时间等工艺参数对双相钢微观组织和力学性能的影响.试验结果表明:试验用钢在820~850℃退火,保温100s以上,抗拉强度可以达到800 MPa级以上.随着退火温度的升高......
,Changsha 410083, P. R. China) 摘要:Three Al-Cu-Mg-Fe-Ni-Sc-Zr ingot metallurgy alloys with different compositions had been prepared. The hardness variations of cold-rolled alloy plates during annealing.... It was found that the dispersed Al3(Sc, Zr) particles could pin dislocations, stabilize substructures and impede the movement of boundaries. The ambient and elevated temperature properties of alloy with Al3......
for the temperature difference control and the type selection of roller in the heating and rapid cooling sections. Key words: continuous annealing furnace; roller; thermal deformation; temperature... in continuous annealing furnace TANG Di, YANG Jing, SU Lan, JIANG Hai-tao, YANG Quan (National Engineering Research Center of Advanced Rolling, University of Science and Technology Beijing, Beijing 100083......
J. Cent. South Univ. (2018) 25: 961-975 DOI: https://doi.org/10.1007/s11771-018-3797-5 Effect of annealing treatment on microstructure and fatigue crack growth behavior of Al–Zn–Mg–Sc–Zr alloy CHEN... (EBSD), transmission electron microscopy (TEM), scanning electron microscopy (SEM), tensile and fatigue crack growth rate tests to explore the influence of annealing treatment on microstructure......
J. Cent. South Univ. Technol. (2009) 16: 0541-0545 DOI: 10.1007/s11771-009-0090-7 Influence of surface finish and annealing treatment on oxidation behavior of Ti-48Al-8Cr-2Ag alloy XI Yan-jun...; Abstract: The effect of surface finish and annealing treatment on the oxidation......
was started in β-phase region and finished in high (α+β)-phase region. Annealing after forging was performed in low (α+β)-phase region for 30 min. Isothermal high temperature compression tests were conducted... Influence of Sc on high temperature strengthening behavior of Ti-6Al-4V alloy LIU Hui-qun(刘会群)1, YI Dan-qing(易丹青)1, WANG Wei-qi(王韦琪)2, WANG Li-ping(王立平)2, LIAN Cai-hao(廉才浩)1 1. School......
magnet was annealed at 3Pa and 492℃ for an hour the coercive force would raise from 915.6kA/m to 1164.8kA/m, and the (BH)max from 277.7kJ/m to 349.5kJ/m. However, annealing at a non-optimized temperature...Effect of Annealing on the Magnetism of the Sintered NdFeB Magnet HUANG Jian-guo1,ZHENG Hua-jun1,MA Chun-an1 (1.College of Chemical Engineering and Material Science, Zhejiang University......