of composites to 500 ℃ occurred in less than 4 min after pressurizing the melt. The samples obtained were of cylindrical shape with a diameter of 5 mm and a height of 20 mm. A detailed description of gas... Microstructure and thermal expansion of Ti coated diamond/Al composites YANG Bo(杨 博), YU Jia-kang(于家康), CHEN Chuang(陈 闯) State Key Laboratory of Solidification Processing, Northwestern......
Polymer-infiltrated layered silicates for dental restorative materialsBen-Cang Cui1,Jing Li1,Yuan-Hua Lin1,Yang Shen1,Ming Li1,Xu-Liang Deng2,Ce-Wen Nan11. State Key Laboratory of New Ceramics and Fine Processing, School of Materials Science and Engineering,Tsinghua University2. School and Hospital of Stomatology,Peking University摘 要:Layered porous......
Hot spinning of cylindrical workpieces of TA15 titanium alloyXU Wenchen,SHAN Debin,YANG Guoping,CHEN Yu,LU Yan,and KANG Dachang School of Materials Science and Engineering,Harbin Institute of Technology,Harbin 150001,China摘 要:In order to form large-diameter thin-wall cylindrical workpieces of TA15 titanium alloy,tube hot spinning experiments......
Heat Dissipation Performance of Porous Copper with Elongated Cylindrical PoresHao Du1,Dongzhu Lu1,Jianzhong Qi1,Yanfang Shen1,Lisong Yin2,Yuan Wang3,Zhongguang Zheng1,Tianying Xiong11. Division... of porous copper with long cylindrical pores fabricated by a unidirectional solidification method.Three samples with porosity of 29.87%,34.47%and 50.98%were chosen and cut into size of 60 mm(length)26......
Tribological characteristics of C/C-SiC braking composites under dry and wet conditions LI Zhuan(李 专)1, XIAO Peng(肖 鹏)1, XIONG Xiang(熊 翔)1, 2, ZHU Su-hua(朱苏华)2 1. State Key Laboratory of Powder...; Abstract: C/C-SiC braking composites, based......
The Failure Mechanisms of Ultra-high Molecular Weight Polyethylene Fibre Composites Under In-plane Compression刘国亮1,2,张玉武31. College of Textile and Clothing, Yancheng Institute of Technology2. Faculty... characteristics of the ultra-high molecular weight polyethylene(UHMWPE) fibre(Dyneema?) reinforced composites, both in 0/90° and ±45° fibre orientations with respect to the loading direction, have been......
mixtures were compacted at a pressure of 200 MPa to get cylindrical blocks (d20 mm×45 mm). Then the composites were sintered at 1 050-1 400 ℃ for 4 h in nitrogen... and sintering dynamics of 10NiO-NiFe2O4 composites doped with CaO LI Jie(李 劼), ZHANG Gang(张 刚), LAI Yan-qing(赖延清), ZHANG Yong(张 勇), TIAN Zhong-liang(田忠良) (School of Metallurgical......
......
......
......