共搜索到18983条信息,每页显示10条信息,共1899页。用时:0小时0分0秒400毫秒
......
of Mechanical Engineering, Tsinghua University, Beijing 100084, China) Abstract:The phosphide eutectic formation process in high purity Fe-4.6%C alloy, in which 0.02%~1.0%P was added, was studied with DTA, SEM and EDS, and the effect of cerium on the morphology of phosphide eutectic in the ternary Fe-C-P alloy was also investigated. The results show that the ternary phosphide eutectic......
......
.......
......
Phase selection in highly undercooled Fe-B eutectic alloy melts
YANG Chang-lin(杨长林), YANG Gen-cang(杨根仓), LU Yi-ping(卢一平),
CHEN Yu-zeng(陈豫增), ZHOU Yao-he(周尧和)
State Key Laboratory... by controlling phase selection in the undercooled melts.
Key words: Fe-B eutectic alloy; metastable phase; phase selection; hypercooling
℃. Copper content has a great influence on the evolution of the eutectic. The coarse phases dissolve slowly in alloy with higher copper content.
Key words: Al-Zn-Mg-Cu alloy; Al2CuMg phase; eutectic... of the 7000 series aluminium alloys[1]. In order to decrease the micro- segregation and dissolve the eutectic, homogenization is necessary for as cast alloy before subsequent processing. Some coarse......Evolution of eutectic structures in Al-Zn-Mg-Cu alloys during heat treatment
AI导读
来源: 《中国有色金属学报(英文版)2006年第3期》——樊喜刚 蒋大鸣 孟庆昌 张宝友 王涛
Solidification structure of eutectic Al-Si alloy under a high magnetic field-aid-electromagnetic vibration Yunbo ZHONG1,Kang DENG1,Weili REN1,Zhongming REN1,Jianbo YU1 (1.Department of Materials...) and an alternative electricity current to the metal.Its effects on the solidification structure of eutectic A1-Si alloy have been investigated experimentally. It is found that the eutectic structure has been......
Microstructure and properties of β-NiAl and its eutectic alloy with Cr and Mo additions ZHANG Zhi-gang(张志刚), LIU Xian-bin(刘先斌), GONG Sheng-kai(宫声凯), XU Hui-bin(徐惠彬) School of Materials Science... alloying with Mo and Cr additions. Key words: β-nickel aluminide; eutectic alloy; compressive properties; brittleness; ductility; fracture morphology 1 Introduction NiAl intermetallic alloys have......
Trans. Nonferrous Met. Soc. China 22(2012) 1582-1587 High temperature oxidation behavior of directionally solidified NiAl-31Cr-2.9Mo-0.1Hf-0.05Ho eutectic alloy WANG Zhen-sheng1,2, XIE Yi2,3, GUO... 2012 Abstract: The isothermal oxidation behavior of NiAl-31Cr-2.9Mo-0.1Hf-0.05Ho directional eutectic alloy was investigated with the help of scanning electron microscopy and X-ray diffraction......