简介概要

Purification technology of AZ91 magnesium alloy wastes

来源期刊:中国有色金属学报(英文版)2003年第6期

论文作者:吴国华 谢敏 翟春泉 曾小勤 朱燕萍 丁文江

文章页码:1260 - 1264

Key words:magnesium alloy; purification; flux; structure; TiO2

Abstract: The effects of different purification processes on the mechanical properties, structure and fracture pattern of AZ91 magnesium alloy wastes were studied. The results show that the inclusions in the Mg melt can be removed effectively by the treatment of the fluxes with MgO foam ceramic filter. Therefore, the properties of magnesium alloy wastes can be improved substantially. Tensile strength and elongation of the magnesium alloy wastes after purification treatment can reach 194.6MPa and 5.12% respectively, which are comparable to the mechanical properties of AZ91 fresh stuff. The metallographic analysis results show that the purification treatment has not obvious effect on metallurgical structure. The fracture mechanism of AZ91 is not changed, and its fractures are still quasi-cleavage crack. It is discovered that for AZ91 magnesium alloy, the fluxes containing TiO2 can decrease the Fe content of magnesium alloy wastes to below 0.0056%. The results also show that TiO2 is helpful for the precipitation of γ phase in granular or small island shape and can refine the grain size effectively.

详情信息展示

 

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号