简介概要

利用反应热处理制备纳米晶 WC-10Co复合粉末

来源期刊:中南大学学报(自然科学版)2003年第5期

论文作者:曹顺华 高海燕 李元元 李炯义 曲选辉

文章页码:480 - 483

关键词:反应热处理;纳米晶复合粉末; WC-Co硬质合金

Key words:reaction thermal treatment; nano-grained composite powder; WC-Co hard metal

摘    要:对反应热处理技术(即高能球磨+热处理)合成纳米晶WC-10Co复合粉末的工艺进行了研究.DTA和X-ray衍射分析结果表明:以W,Co粉和碳黑为原料的混合物经过一定的活化处理后,碳化钨可在572℃左右形成;当温度为800~1 100℃,热处理时间为15~35 min时,合成的纳米碳化钨晶粒尺寸为9~42 nm.反应热处理技术是合成纳米晶WC-Co复合粉末的一种可行的方法.

Abstract: A reaction thermal treatment technique was developed for synthesizing nano-grained WC-10Co composite powders, and the effect of the corresponding processing parameters, such as thermal treatment temperature and time, on the phase formation and the WC grain size was investigated. DTA and XRD analysis results reveal that nano-grained WC can be synthesized at about 572℃.The WC grain size in the synthesized composite powders varies within the range of 9-42 nm when the reaction thermal treatment temperatures and time are adjusted respectively in the range of 15-35 min and in the rage of 800-1 100℃, and the results of the present study indicate that the reaction thermal treatment is an effective technical path to fabricate nano-grained WC-Co powders.

详情信息展示

<上一页 1 下一页 >

相关论文

  • 暂无!

相关知识点

  • 暂无!

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号