氧化铈掺杂氧化锆的等温和非等温马氏体相变(英文)
来源期刊:材料与冶金学报2010年第3期
论文作者:音田哲彦 原纯平 陈中春 早川元造
文章页码:211 - 216
摘 要:Martensitic transformation behavior was studied for zirconia containing 4%~10% CeO2 (in mole fraction) by using a dilatometric method. The Ms (Martensite start temperature) decreased near linearly with increasing CeO2. Different transformation modes were observed depending on the composition and cooling rate. ZrO2 containing 6% CeO2 showed isothermal transformation behavior, whereas ZrO2 containing 9% and 10% CeO2 showed athermal transformation behavior. However, ZrO2 containing 8% CeO2 showed either isothermal or athermal transformations behavior depending on the cooling rate. A TTT (Time-Temperature-Transformation) diagram was proposed for ZrO2 containing 8% CeO2.
音田哲彦1,原纯平2,3,陈中春1,早川元造1
1. 日本鸟取大学2. Graduate Student of Mechanical and Aerospace Engineering,Tottori University
摘 要:Martensitic transformation behavior was studied for zirconia containing 4%~10% CeO2 (in mole fraction) by using a dilatometric method. The Ms (Martensite start temperature) decreased near linearly with increasing CeO2. Different transformation modes were observed depending on the composition and cooling rate. ZrO2 containing 6% CeO2 showed isothermal transformation behavior, whereas ZrO2 containing 9% and 10% CeO2 showed athermal transformation behavior. However, ZrO2 containing 8% CeO2 showed either isothermal or athermal transformations behavior depending on the cooling rate. A TTT (Time-Temperature-Transformation) diagram was proposed for ZrO2 containing 8% CeO2.
关键词: