Glass Formability and Soft Magnetic Properties of Bulk Y-Fe-B-Ti Metals
来源期刊:材料科学与工程学报2007年第6期
论文作者:C. W. Chang C. H. Chiu H. W. Chang Y. C. Huang W. C. Chang
关键词:bulk amorphous; YFeB; Ti effect;
摘 要:The Ti effects on the glass forming ability and the magnetic properties of Y-Fe-B-Ti bulk metallic glasses have been investigated. Substituting 2 and 4 at% Ti for Fe or B in Y6Fe70B22 alloys decrease the saturation magnetization (σs) and deteriorate the glass forming ability, respectively. However, substitution of 2 at% Ti for Y in Y6Fe72B22 alloy induces larger supercooled region of 72.7℃, which not only makes the bulk glassy rod as large as 3mm in diameter, but also results in the superior soft magnetic properties of σ5=126emu/g,coercivity ( Hc ) = 0.2 Oe and Curie temperature (Tc) = 268℃. Among all Y-Fe-B-Ti bulk amorphous rods, Y4Fe72B22Ti2 displays the best glass forming ability and also the proper soft magnetic properties.
C. W. Chang1,C. H. Chiu1,H. W. Chang1,Y. C. Huang1,W. C. Chang1
(1.Physics Department, National Chung Cheng University, Ming-Hsiung, Chia-Yi, Taiwan, China;
2.Institute of Physics, Academia Sinica, Nankang, Taipei, China)
摘要:The Ti effects on the glass forming ability and the magnetic properties of Y-Fe-B-Ti bulk metallic glasses have been investigated. Substituting 2 and 4 at% Ti for Fe or B in Y6Fe70B22 alloys decrease the saturation magnetization (σs) and deteriorate the glass forming ability, respectively. However, substitution of 2 at% Ti for Y in Y6Fe72B22 alloy induces larger supercooled region of 72.7℃, which not only makes the bulk glassy rod as large as 3mm in diameter, but also results in the superior soft magnetic properties of σ5=126emu/g,coercivity ( Hc ) = 0.2 Oe and Curie temperature (Tc) = 268℃. Among all Y-Fe-B-Ti bulk amorphous rods, Y4Fe72B22Ti2 displays the best glass forming ability and also the proper soft magnetic properties.