简介概要

Preparation and Characterization of Low Density Poly (Imino Imino Ketone) Foam

来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2016年第3期

论文作者:刘思曼 常冠军 LUO Meiming

文章页码:700 - 704

摘    要:Poly(Imino Ketone)(PIK) is a group of novel high performance polymer material with excellent thermal properties and dissolubility. Aiming at the requirements of inertial confined fusion(ICF) studies on low density polymer foams, we firstly synthesized poly(imino imino ketone)(PIIK) by palladium catalyzed C-N cross-coupling reaction, and successfully prepared the PIIK foam material with a density of 80-300 mg/cm3 by using PIIK as the raw material with thermal-induced phase separation and lyophilization technique. Mercury injection method was used to determine the structure of PIIK foams, and the results indicated that the mean pore diameter was lower than 5 μm and it had relatively high voidage and specific surface area.

详情信息展示

Preparation and Characterization of Low Density Poly (Imino Imino Ketone) Foam

刘思曼1,常冠军2,LUO Meiming3

1. Department of Chemistry and Chemical Engineering, Mianyang Normal University2. State Key Laboratory Cultivation Base for Nonmetal Composite and Functional Materials & School of Material Science and Engineering, Southwest University of Science and Technology3. Key Laboratory of Green Chemistry & Technology of Ministry of Education, College of Chemistry, Sichuan University

摘 要:Poly(Imino Ketone)(PIK) is a group of novel high performance polymer material with excellent thermal properties and dissolubility. Aiming at the requirements of inertial confined fusion(ICF) studies on low density polymer foams, we firstly synthesized poly(imino imino ketone)(PIIK) by palladium catalyzed C-N cross-coupling reaction, and successfully prepared the PIIK foam material with a density of 80-300 mg/cm3 by using PIIK as the raw material with thermal-induced phase separation and lyophilization technique. Mercury injection method was used to determine the structure of PIIK foams, and the results indicated that the mean pore diameter was lower than 5 μm and it had relatively high voidage and specific surface area.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号