Diffusive healing of internalfatigue micro-cracks in pure titanium

来源期刊:中国有色金属学报(英文版)2001年第5期

论文作者:杨君刚 孙军 张海龙

文章页码:675 - 680

Key words:pure titanium; internal fatigue micro-crack; diffusive healing

Abstract: The internal micro-cracks with the critical length about 30μm and thickness less than 1μmwere introduced into the pure titanium samples by uniaxial tension-compression low cycle fatigue method. The experimental results indicate that the internal fatigue micro-crack clearly evolves from the original penny-shaped crack into a string of spherical voids in the longitudinal section plane of the fatigue sample after the vacuum diffusive healing at the high temperature. The quantitative relationship between the radius and the spacing of spherical voids depends on the crack position (within grains, on grain boundaries or transgranular sites) and its orientations within the grain. The diffusive healing, the related thermodynamics and mechanism, and the effect of the surface tension anisotropy on the relationship between void diameter and void spacing are also discussed.

详情信息展示

 

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号