Preparation of High Molecular Weight Poly(L-lactide-co-caprolactone)(85-15)

来源期刊:Journal Of Wuhan University Of Technology Materials Science Edition2013年第1期

论文作者:湛雪辉 申雄军 LI Zhaohui LI Xia CAO Fen

文章页码:139 - 143

摘    要:Poly(L-lactide-co-caprolactone)(85-15)[P(LLA-CL)(85-15)] was synthesized from high purity L-lactide and ε-caprolactone using tin octoate as initiator by ring-opening polymerization, and characterized by infrared spectrum and 1H-NMR spectrum. The synthesized P(LLA-CL)(85-15) is a random copolymer. The influences of polymerization temperature, polymerization time, dosage of initiator and polymerization pressure on the weight average molecular weight and the polydispersity index of P(LLA-CL)(85-15) were investigated. The optimum preparation conditions of P(LLA-CL)(85-15) are: the polymerization pressure is less than 0.5 Pa, the polymerization temperature is 130 ℃, the n(M)/n(I) ratio is 8 000/1, and the polymerization time is 36 h. Under the condition, the weight-average molecular weight of prepared P(LLA-CL)(85-15) is 65.6×104, and molecular weight distribution coefficient is 1.15.

详情信息展示

Preparation of High Molecular Weight Poly(L-lactide-co-caprolactone)(85-15)

湛雪辉,申雄军,LI Zhaohui,LI Xia,CAO Fen

School of Chemical and Biological Engineering, Changsha University of Science and Technology

摘 要:Poly(L-lactide-co-caprolactone)(85-15)[P(LLA-CL)(85-15)] was synthesized from high purity L-lactide and ε-caprolactone using tin octoate as initiator by ring-opening polymerization, and characterized by infrared spectrum and 1H-NMR spectrum. The synthesized P(LLA-CL)(85-15) is a random copolymer. The influences of polymerization temperature, polymerization time, dosage of initiator and polymerization pressure on the weight average molecular weight and the polydispersity index of P(LLA-CL)(85-15) were investigated. The optimum preparation conditions of P(LLA-CL)(85-15) are: the polymerization pressure is less than 0.5 Pa, the polymerization temperature is 130 ℃, the n(M)/n(I) ratio is 8 000/1, and the polymerization time is 36 h. Under the condition, the weight-average molecular weight of prepared P(LLA-CL)(85-15) is 65.6×104, and molecular weight distribution coefficient is 1.15.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号