Effects of Cooling Paths on Through-Thickness Microstructure and Mechanical Properties of Heavy Gauge X80 Pipeline Steel

来源期刊:Acta Metallurgica Sinica2017年第5期

论文作者:Xu-Dong Li Cheng-Ning Li Guo Yuan Guo-Dong Wang

文章页码:483 - 492

摘    要:The effects of various cooling paths on uniformity of through-thickness microstructure and mechanical properties of X80 pipeline steel of 22.0 mm in thickness were studied. The finite difference method was employed to calculate the temperature field during cooling. It was confirmed by the experimental result and temperature field calculation that the optimizing process was achieved by the ultra-fast cooling with medium cooling capacity(cooling rate of *23 K/s)followed by ultimate cooling capacity(cooling rate of *50 K/s). After optimization, the experimental steel displayed much uniform microstructure and the deviation of through-thickness hardness was controlled within 20 HV. In addition,the yield strength, tensile strength and elongation of the experimental steel were 621, 728 MPa and 21.5%, respectively,meeting the requirements of the API standard for X80 pipeline steels.

详情信息展示

Effects of Cooling Paths on Through-Thickness Microstructure and Mechanical Properties of Heavy Gauge X80 Pipeline Steel

Xu-Dong Li,Cheng-Ning Li,Guo Yuan,Guo-Dong Wang

State Key Laboratory of Rolling and Automation,Northeastern University

摘 要:The effects of various cooling paths on uniformity of through-thickness microstructure and mechanical properties of X80 pipeline steel of 22.0 mm in thickness were studied. The finite difference method was employed to calculate the temperature field during cooling. It was confirmed by the experimental result and temperature field calculation that the optimizing process was achieved by the ultra-fast cooling with medium cooling capacity(cooling rate of *23 K/s)followed by ultimate cooling capacity(cooling rate of *50 K/s). After optimization, the experimental steel displayed much uniform microstructure and the deviation of through-thickness hardness was controlled within 20 HV. In addition,the yield strength, tensile strength and elongation of the experimental steel were 621, 728 MPa and 21.5%, respectively,meeting the requirements of the API standard for X80 pipeline steels.

关键词:

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号