SELECTION OF THE PROCESS PARAMETERS FOR BATH AUTOGENOUS SMELTING OF COPPER

来源期刊:中国有色金属学报(英文版)1993年第1期

论文作者:Guo Xianjian

文章页码:27 - 31

Key words:process parameters; copper bath smelting; autogenous smelting

Abstract: The process parameters for bath autogenous smelting of copper were selected based on dynamic analysis of the experimental data and calculation of the mathematical model. Selecting the slag composition of SiO2/Fe=0.80 and CaO%=16. desulphur ratio less than 80 wt.-% in system. and the copper content of matte less than 60 wt.-%, it is able to limit Fe3O4 formation and obtain a high desulphurization. The critical oxygen content of the blast increased with decrease of the sulphur content of the concentrate and increase of copper contents of the matte. If the copper contents of the concentrate are respectively of 30 and 35 wt.-%, the critical oxygen contents of the blast will be 48 and 69 wt.-% respectively. The smelling rate increases linearly with the blast intensity. When the sulphur content of the concentrate is 30 wt.-%, the oxygen content of the blast 70 vol.-% and the copper content of the matte 60 wt.-%, a blast intensityy of 700 Nm3/m2·h results in a smeling rate of 48.81 t/m2·d.

详情信息展示

 

<上一页 1 下一页 >

有色金属在线官网  |   会议  |   在线投稿  |   购买纸书  |   科技图书馆

中南大学出版社 技术支持 版权声明   电话:0731-88830515 88830516   传真:0731-88710482   Email:administrator@cnnmol.com

互联网出版许可证:(署)网出证(京)字第342号   京ICP备17050991号-6      京公网安备11010802042557号