Dehydrogenation characteristic of Zr1-xMxCo (M=Hf, Sc) alloy
来源期刊:中国有色金属学报(英文版)2007年增刊第1期(Part ⅡB)
论文作者:谭功理 刘晓鹏 蒋利军 王树茂 李志念 李华玲
文章页码:949 - 953
Key words:hydrogen storage alloy; ZrCo; Zr1-xHfxCo; Zr1-xScxCo; intermetallic compound
Abstract: The intermetallic compound Zr1-xHfxCo and Zr1-xScxCo (x=0, 0.1, 0.2, 0.3) were prepared and their suitability for hydrogen storage was investigated. The alloys show single cubic phase identical with ZrCo by X-ray diffraction. Pressure- composition-temperature(PCT) measurement results show that the equilibrium dehydrogenation pressure of Zr1-xHfxCo alloy increases obviously with increasing Hf content while it, changes little with increasing Sc content for Zr1-xScxCo alloy. The dehydrogenation temperatures for supplying 100 kPa hydrogen are about 673, 627, and 650 K for ZrCo, Zr0.7Hf0.3Co and Zr0.7Sc0.3Co alloy, respectively. Thermodynamics calculation results indicate that dehydrogenation ΔH for Zr1-xHfxCo alloy decreases with increasing Hf content but increases with increasing Sc content for Zr1-xScxCo alloy, which are coincident with their dehydrogenation property. The maximal hydrogen storage capacity of both Zr1-xHfxCo and Zr1-xScxCo alloy at room temperature are high enough.